| 溶胶-凝胶法TiO_2涂层碳纤维增强铝基复合材料 |
| 曾庆冰 |
| 第一军医大学;广州;510515 |
|
| FABRICATION OF TiO_2 COATED C_f/ Al BY USING SOL-GEL TECHNIQUE |
| ZENG Qingbing(The First MedicaI University of PLA; Guangzhou 510515) |
引用本文:
曾庆冰. 溶胶-凝胶法TiO_2涂层碳纤维增强铝基复合材料[J]. 金属学报, 1997, 33(9): 1002-1008.
.
FABRICATION OF TiO_2 COATED C_f/ Al BY USING SOL-GEL TECHNIQUE[J]. Acta Metall Sin, 1997, 33(9): 1002-1008.
1Jurek K,Guglielmi M,Kuncova G Renner O,Lukes F,Navratil M,Krousty E Vorlicek V,Kokesova K.J Mater Sci,1992;27:2549 2Helmer T,Peterlik H Kromp K J Am Ceram Soc,1995;1:133 3Von Thicle K H,Panse M.Z Anorg Allg Chem,1978;441:23 4Marrcus H L.AD-A127590, 1983 5Harding J, Welsh L M.J Mater Sci,1983;18:1810 6Huang S C,Hall E L,Gigliotti M F X.J Mater Res ,1988;3:1 7王尊德,刘宗荣,姚忠凯,姚枚.材料科学进展,1993;7:45 |
|