| 异步轧制取向硅钢中织构沿板厚的分布与发展 |
| 刘刚;王福;齐克敏;刘桂兰;梁志德 |
| 东北大学;沈阳;110006;辽宁大学;沈阳;110036;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006 |
|
| TEXTURE DISTRIBUTION AND DEVELOPMENT THROUGH THE THICKNESS AFTER CROSS SHEAR ROLLING OF GRAIN ORIENTED SILICON STEEL |
| LIU Gang (Northeastern University; Shenyang 110006; Liaoning University);Shenyang 110036); WANG Fu; QI Kemin;;LIU Guilan; LIANG Zhide (Northeastern University; Shenyang 110006)(Manuscript received 1996-03-20; in revised form 1996-07-10) |
引用本文:
刘刚;王福;齐克敏;刘桂兰;梁志德. 异步轧制取向硅钢中织构沿板厚的分布与发展[J]. 金属学报, 1997, 33(4): 364-369.
,
,
,
,
.
TEXTURE DISTRIBUTION AND DEVELOPMENT THROUGH THE THICKNESS AFTER CROSS SHEAR ROLLING OF GRAIN ORIENTED SILICON STEEL[J]. Acta Metall Sin, 1997, 33(4): 364-369.
1Goss N P.Trans Am Soc Met,1935;23:511 2米泉.钢铁,1980;15(6):1 3刘刚,王彤,王福,齐克敏,梁志德,栗守维,叶久美。电工钢,1995;4:22 4Liu G,Wang F,Qi K M,Liang Z D.Proc 11th Inte Conf on Textures of Materials,Xi’an,China1996:315 5Liang Z,Xu J,Wang F.Proc 6th Int Conf on Textures of Materials,Tokyo:ISIJ,1981:1259 6梁志德,徐家桢,王福。织构材料的三维取向分析术-ODF分析。沈阳:东北工学院出版社,1986;115:151 7罗阳。金属学报,1977;13(1,2):93 8罗阳,吕其春。金属学报,1979;15:235 9Mishra S,Darmann C,Lucke K.Acta Metall,1984; 32:2185 10刘燕声,梁志德.科学通报,1989;34:471 11刘燕声,赵骧,梁志德。金属学报,1990;25:B198 12朱泉等。板材异步轧制理论与实际。沈阳:东北工学院出版社,1984:48 13Bottcher A,Hastenrath M,Lucke K.Textures Microstruct,1991;(14-18):799 |
|