| γ—TiAl合金拉伸形变的热激活参量 |
| 王瑜;林栋梁;C.C.Law |
| 上海交通大学国家教委高温材料及高温测试开放实验室;上海;200030;上海交通大学国家教委高温材料及高温测试开放实验室;上海;200030;Materials&MechanicsEngineering;UnitedtechnologiesCoporation-Pratt&;06108;USA |
|
| THERMAL ACTIVATION PARAMETERS OF TENSILE DEFORMATION OF GAMMA TITANIUM ALUMINIDE |
| WANG Yu;LIN Dongliang(The Public Laboralory of State Education Commission for High Temperature Materials and High Temperature Tests; Shanghai Jiaotong University; Shanghai 200030); C.C. Law(Materials and Mechanics Engineering; United Technologies Coporalion-Pratt & Whitney; East Hartford; CT 06I08; USA) |
引用本文:
王瑜;林栋梁;C.C.Law. γ—TiAl合金拉伸形变的热激活参量[J]. 金属学报, 1997, 33(11): 1171-1181.
,
,
.
THERMAL ACTIVATION PARAMETERS OF TENSILE DEFORMATION OF GAMMA TITANIUM ALUMINIDE[J]. Acta Metall Sin, 1997, 33(11): 1171-1181.
1KimY—W.JOM,1989;41(7):24 2KimY—W.JOM,1994;46(7):30 3YamaguchiM,InuiH.StructuralIntermetallics.Warrendale,PA:TMS,1993:127 4HuangSC,HallEL.MetallTrans,1991;A22:427 5KumpfertJ,KimY—W,DimidukDM.MaterSciEng,1995;A192/193:465 6ChanKS,KimY-WMetallTrans,1993;A24:114 7MorrisMA,LipeT.ScrMetallMater,1994;31:689 8AppelF,SparkaV,WagnerR.MaterResSocSympProc,1995;364:623 9AppelF,WagnerR.In:KimY—W,WagnerR,YamaguchMeds,GammaTitaniumAluminides,TMS,1995:231 10ViguierB,BonnevilleJ.MaterResSocSympProc,1995;364:629 11ViguierB,CieslarM.MaterResSocSympProc,1995;364:653 12ViguierB,CleslarM.In:KimY—W,WagnerR,YamaguchMeds,GammaTitaniumAluminides,TMS,1995:275 13SchoeckG.PhysStatusSolidi,1965;8:499 14SurekT,LutonMJ,JonasJJ.PhilosMag,1994;A69:105 15SchafrikRE.MetallTrans,1977;A8:1003 16GuiuF,PrattPL.PhysStatusSolid,1964;6:111 17LinDongliang,Wangyu,LawCC.MaterSciEng(A),tobePublished18EzzSS,HirschPB.PhilosMag,1994;A69:105 19ConradH.JOM,1964;16:582 20HallEQ.ProcPhysSoc,1951;B64:747 21PetchNJ.JIronSteelInst,1953;174:25 22KrollS,MehrerH,StolwijkN,HerzigC,RosenkranzR,FrommeyerG.ZMettallkd,1992;83:591 23SprengelW,OikawaN,NakajimaH.Intermetallics,1996;4:185 24王瑜,林栋梁.金属学报,1997;33:1021 25JonasJJ,LutonMJ.MetallTrans,1971;2:3492 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|