| 铜熔炼过程中伴生元素分配行为的计算机模型 |
| 谭鹏夫;张传福 |
| 中南工业大学;长沙410083;中南工业大学;长沙410083 |
|
| COMPUTER MODEL OF DISTRIBUTION BEHAVIOR OF ACCESSORY ELEMENTS IN COPPER SMELTING |
| TAN Pengfu;ZHANG Chuanfu(Central South University of Technology; Changsha 410083) |
引用本文:
谭鹏夫;张传福. 铜熔炼过程中伴生元素分配行为的计算机模型[J]. 金属学报, 1997, 33(10): 1094-1100.
,
.
COMPUTER MODEL OF DISTRIBUTION BEHAVIOR OF ACCESSORY ELEMENTS IN COPPER SMELTING[J]. Acta Metall Sin, 1997, 33(10): 1094-1100.
1 Itagaki K, Yazawa a. In:Sohn H Y, ed., advances in Sulfide Smelting. Utah: americal Institute ofMining, Metallurgical and Petroleum Engineers, 1983:119 2 Chaubal P C. MetalI Trans, 1989; 20B(12):39 3 Shimpo R, Ogawa O, Goto S. Metall Trans, 1993, 24a(8):1882 4 Shimpo R, Watanabe Y, Goto S. In. Sohn H Y, ed., advances in Sulfide Smelting. Utah:americalInstitute of Mining, Metallurgical and Petroleum Engineers, 1983; 295 5 Nagamori N, Mackey P J. Metall Trans, 1978; 9B:567 6 Nagamori M, Errington W J, Mackey P J. MetalI Trans. 1994; 25B(12):839 7 Seo K W, Sohn H Y. Metall Trans. 1991; 22B(12):791 8 Yazawa a, Nakazawa S, Takeda Y. In:Sohn H Y, ed., advances in Sulfide Smelting. Utah:americal Institute of Mining, Metallurgical and Petroleum Engineers, 1983; 90 9 Sinha S N, Nagamori M. Metall Trans. 1982, 13B(9). 461 10 Sinha S N, Sohn H Y, Nagamori M. Metall Trans. 1984; 15B(9):595 11 Sinha S N, Sohn H Y, Nagamori M. Metall Trans. 1985; 16B(31):53 12 Takeda Y, Ishinata S, Yazawa a. Trans Jpn Inst Met, 1983; 24(7):518 13 Mackey P J. Can Metall Q, 1982, 21(3). 221 14 Grimsey E J, Liu X L. Metall Trans, 1995; 26B(4): 229 15 Jalkanen H K, Holppa L E K.In:Sohn H Y,ed,advances in Sulfide Smelting.Utah: americal Institute of Mining,Metallurgical and Petroleum Engineers,1983:277 16Nagamori M, Mackey P J. Metall Trans, 1978; 9B(6): 255 17王震华,有色冶金设计与研究.1993;14(4):18 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|