Please wait a minute...
金属学报  1997, Vol. 33 Issue (10): 1085-1093    
  论文 本期目录 | 过刊浏览 |
高阶亚正规溶液模型及其在MnO-SiO_2-Al_2O_3-CaO炉渣中组元活度的计算
张晓兵;蒋国昌;徐匡迪
上海大学;上海市钢铁冶金新技术开发应用重点实验室;上海200072;上海大学;上海市钢铁冶金新技术开发应用重点实验室;上海200072;上海大学;上海市钢铁冶金新技术开发应用重点实验室;上海200072
HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG
ZHANG Xiaobing;JIANG Guochang;XU Kuangdi (Shanghai University; ShanghaiEnhanced Lab of Ferrometallurgy; Shanghai 200072)
引用本文:

张晓兵;蒋国昌;徐匡迪. 高阶亚正规溶液模型及其在MnO-SiO_2-Al_2O_3-CaO炉渣中组元活度的计算[J]. 金属学报, 1997, 33(10): 1085-1093.
, , . HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG[J]. Acta Metall Sin, 1997, 33(10): 1085-1093.

全文: PDF(709 KB)  
摘要: 本文介绍了用于计算四元均相系中组元活度的SELF-SReM4高阶亚正规溶液模型.模型由一组参数表示,根据精选的“边界条件”.可由二元系、三元系、四元系逐渐展开拟合出该组参数.用该模型计算了Mno-SiO2-al2O3-CaO四元系,包括四个三元子系中各组元的活度.SiO2-al2O3-CaO三元系的SiO2活度计算值与实验值和其它计算结果较一致;MnO-SiO2-CaO三元系计算结果与渣-金属平衡试验结果较一致
关键词 : 高阶亚正规溶液模型,  MnO-SiO_2-Al_2O_3-CaO四元系,  组元活度计算    
Abstract:a high order sub-regular solution modeI for predicting the component activities in a homogeneous region of a quaternary system was developed in the Shanghai Enhanced Lab of Ferrometallurgy, which is designated as SELF-SReM4. It is composed of some polynomials of excess mole free energies versus content variable. a group of parameters is included in the polynomials. along with the reliable known thermodynamic properties associating the homogeneous region the parameters can be evaluated. and then the component activities in that region are possible to be predicated. This paper is devoted to illustrate the applications of SELF-SReM4 for molten slag of MnO-SiO2-al2O3-CaO and its sub-ternary systems. The evaluated results were very close to those of slag-metal equilibrium experiments and the Chipman's and Pelton's results.
Key words: SELF-SReM4 model    MnO-SiO_2-Al_2O_3-CaO system    calculation of component activity
收稿日期: 1997-10-18     
1 Masson V R. 2nd Intern Confon Melten Fluxes and Slags, Lake Tahoe, 1984; 3
2 万谷郎,日野光兀,铁钢,1988, 74;1701
3 Pelton a D, Blander M. 2nd Intern Con fon Melten Fluxes and Slagr, Lake Tahoe, 1984;281
4 Kriksson G, Pelton a D. Metall Trans. 1993, 24B:795
5 Gaye H, Welfringer J. 2nd Intern Confon Melten Fluxes and Slagr, Lake Tahoe, 1984;357
6 Gaye H, Riboud P V, Welfringer J. 5th Int. Iron SteeI Congr, Washington D.C., 1996: 631
7 Hillert M, Jansson B, Sundman B, J agren Met Trans, 1985; 16a:261
8 Jiang Guo Chang, Zhang Xiao Bing, Xu Kuang Di. acla Metall Sin, 1992, 5B:476
9 Zhang Xiao Bing. Ph.D. Thesis, Shanghai University, 1996:24
10 S.Ban-Ya, M.Hino. Chemical Properties of Melten Slags, ISIJ, 1991; 17
11 abraham K P, Davies M W, Richardson F D. J Iron Steel Inst, 1960, 196:82
12 Sharma R a, Richardson F D. Trans MeI Soc aIME, 1965, 233:1586
l3 Rein R H, Chipman J. Trans Met Soc aIME, 1965, 233; 415
14 Sharma R a, Richardson F D. J Iron Steel Inst, 1961, 198:386
15 Risbud S H, Pask J a. J am Ceramic Society, 1977, 60, 418
16 Mehta S R, Richardson F D. J Iron Steel Inst, 1965, 203:524
17 Warren G F, Jochens P R, Howat D D. INFaCON, 1974: 175
18 Ding W, Olsen S E. Metall Trans, 1996; 27B:5
No related articles found!