| 用ODF理论研究Fe-30Ni合金α-γ_r逆相变过程的织构变化 |
| 孙丽娟;刘维鹏 |
| 北京航空航天大学;北京工业大学 |
|
| STUDY OF(α-γ_r) REVERSE TRANSFORMATION TEXTURE IN Fe-30Ni ALLOY BY USE OF ODF THEORY |
| SUN Lijuan (Beijing University of Aeronautics and Astronautics; Beijing 100083); LIU Weipeng (Beijing Polytechnic University; Beijing 100022)H J Bunge (Department of Physical Metallurgy; TU Clausthal FRG) |
引用本文:
孙丽娟;刘维鹏. 用ODF理论研究Fe-30Ni合金α-γ_r逆相变过程的织构变化[J]. 金属学报, 1996, 32(9): 913-920.
,
.
STUDY OF(α-γ_r) REVERSE TRANSFORMATION TEXTURE IN Fe-30Ni ALLOY BY USE OF ODF THEORY[J]. Acta Metall Sin, 1996, 32(9): 913-920.