| EFFECTS OF HEAT TREATMENT ON Pb-DOPED Bi-2223 SUPERCONDUCTOR |
| ZHANG Liuwan; CHEN Tingguo; XIE Xiaoming; WU Xiaochu; SHITiansheng(Shanghai Institute of Metallurgy; Chinese Academy of Sciences;Shanghai 200050) LI Xiangting; GAO Jianhua; SUN Jing(Shanghai Institute of Ceramics;Chinese Academy of Sciences; Shanghai 200050) |
引用本文:
张留琬;陈廷国;谢晓明;吴晓初;施天生;李香庭;高建华;孙荆. 热处理对Bi-Pb-Sr-Ca-Cu-O超导材料结构和超导性能的影响[J]. 金属学报, 1995, 31(6): 277-285.
,
,
,
,
,
,
,
.
EFFECTS OF HEAT TREATMENT ON Pb-DOPED Bi-2223 SUPERCONDUCTOR[J]. Acta Metall Sin, 1995, 31(6): 277-285.
| 1IwaiY,HoshiY,SaitoH,TakataM.PhysicaC,1990;170:3192张留琬,陈廷国.物理学报待发表3TakedaY,KannoR,TanigawaF,YamamotoO,IkedaY,TakanoM.PhysicaC,1989;159:7894IdemotoY,FujiwaraS,FuekiK.PhysicaC,1991;179:965XieXM,ZhangLW,ChenTG.PhysicaC,1993;206:2516ZhouCJ,LiTW,ChenTG.PhysicaC,1991;179:3697沈忠哲.中国科学院上海冶金研究所硕士学位论文,19928MatsuiY,MaedaH,TanakaY,HoriuchiS.JpnJApplPhys,1988;27:L3619ZandbergenHW,GroenWA,VanTendelooGvan,VanLandugtJ,AmelinckxS.SolidStateCommun,1988;66:39710ShawTM,ShivashankarSA,LaplacaSJ,GuonnJJ,McguireTR,RoyRA,KelleberKH,YeeDS.PhysRev,1988;B37:985611FukushimaN,NiuH,NakamuraS,TakenoS,HayashiM,AndoK.PhysicaC,1989;159:77712IkedaS,AotaK,HatanoT,OgawaK,JpnJApplPhys,1988;27:L204013RameshR,TendelovGvan,ThomasG,GreenSM,LuoHL.ApplPhysLett,1988;53:2220P |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|