| Na_2SO_4沉积盐引起的Ni_3Al-Fe的中温区热腐蚀 |
| 曾潮流;张鉴清;吴维玟;郭建亭 |
| 中国科学院金属腐蚀与防护研究所腐蚀科学开放研究实验室;中国科学院金属研究所 |
|
| Na_2SO_4 INDUCED HOT CORROSION OF Ni_3Al-Fe INTERMETALLIC COMPOUND AT INTERMEDIATE TEMPERATURES |
| ZENG Chaoliu;ZHANG Jianqing;WU Weitao(Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences ;Shenyang)GUO Jianting (Institute of Metal Research; Chinese Academy of Sciences; Shenyang) |
引用本文:
曾潮流;张鉴清;吴维玟;郭建亭. Na_2SO_4沉积盐引起的Ni_3Al-Fe的中温区热腐蚀[J]. 金属学报, 1994, 30(21): 398-402.
,
,
,
.
Na_2SO_4 INDUCED HOT CORROSION OF Ni_3Al-Fe INTERMETALLIC COMPOUND AT INTERMEDIATE TEMPERATURES[J]. Acta Metall Sin, 1994, 30(21): 398-402.
| 1李辉,郭建亭,谭明晖,孙超,赖万慧,王淑荷,金属学报,1992;28:A3372沈华清,曾潮流,楼翰一,王福会,郭建亭,吴维.腐蚀科学与防护技术,1993;29:B4503曾潮流,张鉴清,吴维.材料工程,1993;119:14张允书,李连方,石声泰.中国腐蚀与防护学报,1990;10:2755沈华清,曾潮流,吴维,郭建亭.金属学报,1993;29:B4506SternKH,DeanhardtML,PanayappanRm.JPhysChem,1979;83:2848 |
|