| 热变形对合金钢A_(e3)影响的热力学计算 |
| 刘振宇;王国栋;张强;马龙翔 |
| 东北大学 |
|
| THERMODYNAMICAL CALCULATIONS OF INFLUENCES OF HOT-DEFORMATION ON A_(e3) FOR ALLOY STEELS |
| LIU Zhenyu; WANG Guodong; ZHANG Qiang;MA Longxiang(Northeastern University; Shenyang) |
引用本文:
刘振宇;王国栋;张强;马龙翔. 热变形对合金钢A_(e3)影响的热力学计算[J]. 金属学报, 1994, 30(18): 277-282.
,
,
,
.
THERMODYNAMICAL CALCULATIONS OF INFLUENCES OF HOT-DEFORMATION ON A_(e3) FOR ALLOY STEELS[J]. Acta Metall Sin, 1994, 30(18): 277-282.
| 1UmemotoM,TamuraI.ProcofIntConfofHSLASteel'85Beijing,1985:3732AnanGetal,ISIJInternational,1992:32:33AaronsonHI,DomionHA,PoundGM.TransofAIME,1966;236:7534徐祖耀,刘世楷.贝氏体相变与贝氏体.北京:科学出版社,19915ZenerC.TransAIME,1946;167:5136杨柳,刘世楷,杨萍.金属学报,1993;29:Al7AaronsonHI,DomianHA.TransAIME,1966;236:7818GrangeRA,MetalProgress,1961:203:739林慧国,傅代直.钢的奥氏体转变曲线.北京:机械工业出版社,1988 |
|