| 奥氏体-贝氏体球墨铸铁中奥氏体对接触疲劳性能的影响 |
| 丛家瑞;范鹤立;曹兴言;李隆盛;曹月君;徐香秋 |
| 大连理工大学材料系铸工教研室;大连116024;大连理工大学;大连理工大学;大连理工大学;长春汽车材料研究所;长春汽车材料研究所 |
|
| EFFECT OF AUSTENITE ON CONTACT FATIGUE PROPERTIES OF AUSTENITE-BAINITE DUCTILE IRON |
| CONG Jiarui; FAN Heli; CAO Xingyan; LI Longsheng (Dalian University of Technology); CAO Yuejun; XU Xiangqiu (Changchun Automobile Materials Institute) |
引用本文:
丛家瑞;范鹤立;曹兴言;李隆盛;曹月君;徐香秋. 奥氏体-贝氏体球墨铸铁中奥氏体对接触疲劳性能的影响[J]. 金属学报, 1992, 28(7): 41-44.
,
,
,
,
,
.
EFFECT OF AUSTENITE ON CONTACT FATIGUE PROPERTIES OF AUSTENITE-BAINITE DUCTILE IRON[J]. Acta Metall Sin, 1992, 28(7): 41-44.
1 Sharma V K. In: lst Int Conf on Austempered Ductile Iron: Your Means to Improved Performance, Productivily and Cost, Chicago, April 2-4, 1984, ASM, 1984:53-62 2 Kalevi J. In: lst Conf on Austempered Ductile Iron: Your Means to Improved Performance, Productivily and Cost, Chicago, April 2-4, 1984, ASM, 1984: 135-148 3 沈会滨.铸造技术,1986;(6) :31-34 4 曹月君,丛家瑞,徐香秋,范鹤立.球铁,1989;(4) :10-14 5 范鹤立,丛家瑞,李隆盛.大连理工大学学报,1989;29:295-300 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|