| GCr15轴承钢接触疲劳次表面裂纹的跟踪观察 |
| 陈隆庆;陈箐 |
| 郑州工学院;讲师;洛阳工学院 |
|
| TRACKING OBSERVATION ON SUBSURFACE CRACKING IN GCr15 BEARING STEEL UNDER ROLLING CONTACT FATIGUE |
| CHEN Longqing Zhengzhou Institute of Technology; CHEN Qing Luoyang Institute of Technology |
引用本文:
陈隆庆;陈箐. GCr15轴承钢接触疲劳次表面裂纹的跟踪观察[J]. 金属学报, 1991, 27(5): 61-65.
,
.
TRACKING OBSERVATION ON SUBSURFACE CRACKING IN GCr15 BEARING STEEL UNDER ROLLING CONTACT FATIGUE[J]. Acta Metall Sin, 1991, 27(5): 61-65.
1 Yoshimura H, Rubin C A, Hahn G T. Wear, 1984; 95: 29--34 2 Leng Xiaogang, Chen Qing, Shao Eryu. Wear, 1988; 122: 33--43 3 陈隆庆,陈箐,邵尔玉.理化检验(物理分册),1990;26(6) :24-27 4 Chen Longching, Chen Qing, Shao Eryu. Wear, 1989; 133: 205--218 5 陈隆庆,陈箐,邵尔玉.机械工程学报,1991;待发表 6 徐芝纶,弹性力学.北京:人民教育出版社,1979 7 日紫喜基久,堀捷(木鼓),高野博史,川辺秀昭,上村正雄,精密机械,1978;44:1321-1327 8 姜秉元,邵尔玉,金属学报,1986;22:A297-303 9 邵尔玉,王长生,郑世安.洛阳工学院内部资料,1986 |
|