| 下贝氏体铁素体宽面上的台阶结构 |
| 金强;方鸿生;曹建军;郑燕康;陈秀云 |
| 清华大学冶金工业部钢铁研究总院;)清华大学材料科学与工程系;教授;清华大学;清华大学;清华大学 |
|
| LEDGE STRUCTURE AT BROAD FACES OF FERRITE PLATES IN LOWER BAINITE |
| JIN Qiang;FANG Hongsheng;CAO Jianjun;ZHENG Yankang;CHEN Xiuyun Tsinghua University; Beijing |
引用本文:
金强;方鸿生;曹建军;郑燕康;陈秀云. 下贝氏体铁素体宽面上的台阶结构[J]. 金属学报, 1990, 26(6): 5-9.
,
,
,
,
.
LEDGE STRUCTURE AT BROAD FACES OF FERRITE PLATES IN LOWER BAINITE[J]. Acta Metall Sin, 1990, 26(6): 5-9.