| 几种耐磨合金磨损温度场的热图 |
| 黄毅;白元凯;徐军;林雪荣 |
| 中国科学院金属研究所;副研究员;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| TEMPERATURE FIELD THERMOGRAPHY ON FRICTION FACING OF CERTAIN WEAR-RESISTANT ALLOYS |
| HUANG Yi;BAI Yuankai;XU Jun;LIN Xuerong Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
黄毅;白元凯;徐军;林雪荣. 几种耐磨合金磨损温度场的热图[J]. 金属学报, 1990, 26(5): 153-155.
,
,
,
.
TEMPERATURE FIELD THERMOGRAPHY ON FRICTION FACING OF CERTAIN WEAR-RESISTANT ALLOYS[J]. Acta Metall Sin, 1990, 26(5): 153-155.
1 Bowden F P, Tabor D. The Friction and Lubrication of Solids, Part Ⅱ, Oxford: Clarendon Press, 1964: 31 2 黄毅,林雪荣,徐军.金属学报,1988;24:B207 3 Archard J F. Wear, 1958--59; 2: 43 |
|