| Al-Si涂层脆-塑性转变温度对镍基高温合金性能的影响 |
| 张德堂 |
| 北京航空材料研究所 |
|
| EFFECT OF DUCTILE-BRITTLE TRANSITION TEMPERATURE OF Al-Si COATING ON FATIGUE PROPERTIES OF Ni-BASE SUPERALLOYS |
| ZHANG Detang Beijing Institute of Aeronautical Materials |
引用本文:
张德堂. Al-Si涂层脆-塑性转变温度对镍基高温合金性能的影响[J]. 金属学报, 1990, 26(3): 61-65.
.
EFFECT OF DUCTILE-BRITTLE TRANSITION TEMPERATURE OF Al-Si COATING ON FATIGUE PROPERTIES OF Ni-BASE SUPERALLOYS[J]. Acta Metall Sin, 1990, 26(3): 61-65.
1 Wells C H, Sullivan C P. ASM Trans Q, 1968; 61: 149 2 Goward G W. J Met, 1970; 22 (10) : 31 3 Holmes D R, Rahmel A. Materials and Coating to Resist High Temperature Corrosion, London: Applied Science 1978: 233 4 Vogel D J. Naval Postgradute School, Thesis, 1985 5 Paskiet G F, Boone D H. Sullivan C P. J Iust Met, 1972; 100: 58 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|