| Fe-V-Ce溶液的热力学性质研究 |
| 唱鹤鸣;杜挺;余景生 |
| 冶金部钢铁研究总院;北京冶金工业部钢铁研究总院;高级工程师(教授级);冶金部钢铁研究总院 |
|
| THERMODYNAMIC PROPERTIES OF Fe-V-Ce LIQUID SOLUTION |
| CHANG Heming;DU Ting;YU Jingsheng Central Iron and Steel Research Institute; Beijing |
引用本文:
唱鹤鸣;杜挺;余景生. Fe-V-Ce溶液的热力学性质研究[J]. 金属学报, 1989, 25(2): 152-154.
,
,
.
THERMODYNAMIC PROPERTIES OF Fe-V-Ce LIQUID SOLUTION[J]. Acta Metall Sin, 1989, 25(2): 152-154.
1 周谦莉,杜挺,金属学报,1989;25(1) ; 2 Savitskii E M. Baron VV. Efimov Yu V. Eng Transl Russ J Inorg Chem, 1962: 7; 359 3 乐可襄,杜挺,李继宗,沈汝美,金属学报,1987;23:A99 4 Wu Yieming, Wang Longmei, Du Ting. J Less-Common Met, 1985; 110: 187 5 韩其勇,北京钢铁学院学报,1986;(3) :115 6 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298 7 Elliott J F. Electr Furnace Conf Proc, 1974; 32: 62 8 Gibson J. Properties of the Rare Earth Metals and Compounds, 1966: 59~ |
|