| 低碳钢中磷的偏聚与再结晶织构 |
| 张立新;曲哲;李黎光;魏文铎 |
| 副研究员;沈阳中国科学院金属腐蚀与防护研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| PHOSPHORUS SEGREGATION AND ANNEALING TEXTURE IN A LOW CARBON STEEL SHEETS |
| ZHANG Lixin;QU Zhe;LI Liguang;WEI Wenduo Institute of Corrosion and protection of Metals; Academia Sinica; Shenyang; Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
张立新;曲哲;李黎光;魏文铎. 低碳钢中磷的偏聚与再结晶织构[J]. 金属学报, 1988, 24(5): 336-342.
,
,
,
.
PHOSPHORUS SEGREGATION AND ANNEALING TEXTURE IN A LOW CARBON STEEL SHEETS[J]. Acta Metall Sin, 1988, 24(5): 336-342.
1 Mishra S, Darmann C. Int Metall Rev, 1982; 27: 307 2 Takechi H, Abe M. Nippen Steel Tech Rep, 1984; 23: 9 3 Ohashi N, Honishi M, Yasuoa A, Sato S, Irie T. In: Proc 6th Int Conf on Textures of Materials, Tokyo: ISIJ, Vol. I, 1981: 195 4 Matsudo K. Shimomura T, Osawa K, Sakoh M, Ono S. In: Proc 6th Int Conf on Textures of Materials, Vol. Ⅰ, Tokyo: ISIJ, 1981; 259 S Muller M H, et al. Trans AIME, 1958; 212: 39 6 Li Zhengxiu (李正修), Liu Xingpu (刘星浦), Xu Xinhe, (徐心和); Lai Jingyan (来金岩), Control Decision, 1986; 3: 16 7 Liang Zhide (梁志德), Xu Jiazheng (徐家桢), Wang Fu(王福). In: Proc 6th Int Conf on Textures of Materials, Vol. Ⅱ, Tokyo: ISIJ. 1981: 1259Q |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|