纵向磁场对Al-40%Cu过共晶合金定向凝固显微组织的影响 |
沈裕, 任忠鸣, 李喜, 任维丽 |
上海大学上海市现代冶金与材料制备重点实验室, 上海 200072 |
|
EFFECT OF LONGITUDINAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED Al-40%Cu HYPEREUTECTIC ALLOY |
SHEN Yu, REN Zhongming, LI Xi, REN Weili |
Shanghai Key Laboratory of Modern Metallurgy & Materials Processing, Shanghai University, Shanghai 200072 |
引用本文:
沈裕 任忠鸣 李喜 任维丽. 纵向磁场对Al-40%Cu过共晶合金定向凝固显微组织的影响[J]. 金属学报, 2011, 47(4): 417-422.
,
,
,
.
EFFECT OF LONGITUDINAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED Al-40%Cu HYPEREUTECTIC ALLOY[J]. Acta Metall Sin, 2011, 47(4): 417-422.
[1] Shercliff J A. J Fluid Mech, 1979; 91: 231
[2] Moreau R, Laskar O, Tanaka M, Camel D. Mater Sci Eng, 1993; A173: 93
[3] Lehmann P, Moreau R, Camel D, Bolcato R. Acta Mater, 1998; 46: 4067
[4] Yesilyurt S, Vujisic L, Motakef S, Szofran F R, Volz M P. J Cryst Growth, 1999; 207: 278
[5] Li X, Fautrelle Y, Ren Z M. Acta Mater, 2007; 55: 3803
[6] Li X, Gagnoud A, Ren Z M, Fautrelle Y, Moreau R. Acta Mater, 2009; 57: 2180
[7] Yilmaz F, Elliott R. J Cryst Growth, 1984; 66: 465
[8] Li X, Ren Z M, Fautrelle Y. Acta Mater, 2006; 54: 5349
[9] Jin F W. PhD Thesis, Shanghai University, 2007
(晋芳伟. 上海大学博士学位论文, 2007)
[10] Moreau R. Magnetohydrodynamics. Dordrecht: Kluwer Academic Publishers, 1990: 111
[11] Robertson G D, O’Connor D. J Cryst Growth, 1986; 76: 100
[12] Kishida Y, Takeda K, Miyoshino I, Taleuchi E. ISIJ Int, 1990; 30: 34
[13] Laskar O. PhD Thesis, Laboratoire MADYLAM, France, 1994
[14] Callen H B. Phys Rev, 1984; 73: 1349
[15] Li X, Ren Z M, Fautrelle Y, Zhang Y D, Esling C. Mater Lett, 2010; 64: 2597 |
|
Viewed |
|
|
|