Mg中双拉伸孪晶及其构成的复合孪晶结构 |
石章智1,2( ), 刘雪峰1,2,3 |
1 北京科技大学材料科学与工程学院 北京 100083 2 北京科技大学现代交通金属材料与加工技术北京实验室 北京 100083 3 北京科技大学材料先进制备技术教育部重点实验室 北京 100083 |
|
Double Extension Twin and Its Related CompoundTwin Structures in Mg |
Zhangzhi SHI1,2( ), Xuefeng LIU1,2,3 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 Beijing Laboratory of Metallic Materials and Processing for Modern Transportation, University of Science and Technology Beijing, Beijing 100083, China 3 Key Laboratory for Advanced Materials Processing of Ministry of Education, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
石章智, 刘雪峰. Mg中双拉伸孪晶及其构成的复合孪晶结构[J]. 金属学报, 2018, 54(12): 1715-1724.
Zhangzhi SHI,
Xuefeng LIU.
Double Extension Twin and Its Related CompoundTwin Structures in Mg[J]. Acta Metall Sin, 2018, 54(12): 1715-1724.
[1] | Christian J W, Mahajan S.Deformation twinning[J]. Prog. Mater Sci., 1995, 39: 1 | [2] | Partridge P G.The crystallography and deformation modes of hexagonal close-packed metals[J]. Metall. Rev., 1967, 12: 169 | [3] | Tu J, Zhang S Q.On the {10ˉ12} twinning growth mechanism in hexagonal close-packed metals[J]. Mater. Des., 2016, 96: 143 | [4] | Barnett M R, Keshavarz Z, Beer A G, et al.Non-Schmid behaviour during secondary twinning in a polycrystalline magnesium alloy[J]. Acta Mater., 2008, 56: 5 | [5] | Cizek P, Barnett M R.Characteristics of the contraction twins formed close to the fracture surface in Mg-3Al-1Zn alloy deformed in tension[J]. Scr. Mater. 2008, 59: 959 | [6] | Lentz M, Risse M, Schaefer N, et al.Strength and ductility with {1011}-{10ˉ12} double twinning in a magnesium alloy[J]. Nat. Commun., 2016, 7: 11068 | [7] | Martin é, Capolungo L, Jiang L, et al.Variant selection during secondary twinning in Mg-3%Al[J]. Acta Mater., 2010, 58: 3970 | [8] | Agnew S R, Duygulu ?.Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B[J]. Int. J. Plast., 2005, 21: 1161 | [9] | Hutchinson W B, Barnett M R.Effective values of critical resolved shear stress for slip in polycrystalline magnesium and other hcp metals[J]. Scr. Mater., 2010, 63: 737 | [10] | Koike J.Enhanced deformation mechanisms by anisotropic plasticity in polycrystalline Mg alloys at room temperature[J]. Metall. Mater. Trans., 2005, 36A: 1689 | [11] | Xu S, Liu T M, Chen H C, et al.Reducing the tension-compression yield asymmetry in a hot-rolled Mg-3Al-1Zn alloy via multidirectional pre-compression[J]. Mater. Sci. Eng., 2013, A565: 96 | [12] | Song B, Xin R L, Sun L Y, et al.Influencing factors and controlling methods of tension-compression asymmetry in magnesium alloys[J]. Chin. J. Nonferrous Met., 2014, 24: 1941(宋波, 辛仁龙, 孙立云等. 镁合金拉伸压缩不对称性的影响因素及控制方法[J]. 中国有色金属学报, 2014, 24: 1941) | [13] | Shi Z Z, Zhang Y D, Wagner F, et al.Sequential double extension twinning in a magnesium alloy: Combined statistical and micromechanical analyses[J]. Acta Mater., 2015, 96: 333 | [14] | Shi Z Z.Compound cross-grain boundary extension twin structure and its related twin variant selection in a deformed Mg alloy[J]. J. Alloys Compd., 2017, 716: 128 | [15] | Shi Z Z, Xu J Y, Yu J, et al.Intragranular cross-level twin pairs in AZ31 Mg alloy after sequential biaxial compressions[J]. J. Alloys Compd., 2018, 749: 52 | [16] | Godet S, Jiang L, Luo A A, et al.Use of Schmid factors to select extension twin variants in extruded magnesium alloy tubes[J]. Scr. Mater., 2006, 55: 1055 | [17] | Jonas J J, Mu S J, Al-Samman T, et al.The role of strain accommodation during the variant selection of primary twins in magnesium[J]. Acta Mater., 2011, 59: 2046 | [18] | Xin R L, Guo C F, Xu Z R, et al.Characteristics of long {10ˉ12} twin bands in sheet rolling of a magnesium alloy[J]. Scr. Mater., 2014, 74: 96 | [19] | Shi Z Z, Liu X F.Characteristics of cross grain boundary contraction twin pairs and bands in a deformed Mg alloy[J]. J. Alloys Compd., 2017, 692: 274 | [20] | Hong X, Godfrey A, Liu W.Challenges in the prediction of twin transmission at grain boundaries in a magnesium alloy[J]. Scr. Mater., 2016, 123: 77 | [21] | Barnett M R, Nave M D, Ghaderi A.Yield point elongation due to twinning in a magnesium alloy[J]. Acta Mater., 2012, 60: 1433 | [22] | Park S H, Hong S G, Lee J H, et al.Multiple twinning modes in rolled Mg-3Al-1Zn alloy and their selection mechanism[J]. Mater. Sci. Eng., 2012, A532: 401 | [23] | Shi Z Z, Zhang Y D, Wagner F, et al.On the selection of extension twin variants with low Schmid factors in a deformed Mg alloy[J]. Acta Mater., 2015, 83: 17 | [24] | Shi Z Z.Secondary twin variant selection in Mg alloy after a strain-path change[J]. J. Alloys Compd., 2017, 696: 510 | [25] | Jain J, Zou J, Sinclair C W, et al.Double tensile twinning in a Mg-8Al-0. 5Zn alloy[J]. J. Microsc., 2010, 242: 26 | [26] | Mu S J, Jonas J J, Gottstein G.Variant selection of primary, secondary and tertiary twins in a deformed Mg alloy[J]. Acta Mater., 2012, 60: 2043 | [27] | Barnett M R, Stanford N, Ghaderi A, et al.Plastic relaxation of the internal stress induced by twinning[J]. Acta Mater., 2013, 61: 7859 | [28] | Yu Q, Wang J, Jiang Y Y, et al.Twin-twin interactions in magnesium[J]. Acta Mater., 2014, 77: 28 | [29] | Yu Q, Wang J, Jiang Y Y, et al.Co-zone {ˉ1012} Twin interaction in magnesium single crystal[J]. Mater. Res. Lett., 2014, 2: 82 | [30] | Morrow B M, Cerreta E K, McCabe R J, et al. Toward understanding twin-twin interactions in hcp metals: Utilizing multiscale techniques to characterize deformation mechanisms in magnesium[J]. Mater. Sci. Eng., 2014, A613: 365 | [31] | Sun Q, Zhang X Y, Ren Y, et al. Interfacial structure of {10ˉ12} twin tip in deformed magnesium alloy [J]. Scr. Mater., 2014, 90-91: 41 | [32] | Zhang J, Xi G Q, Wan X, et al.The dislocation-twin interaction and evolution of twin boundary in AZ31 Mg alloy[J]. Acta Mater., 2017, 133: 208 |
|
|