1000 MPa级0Cr16Ni5Mo钢的氢脆敏感性研究* |
孙永伟1,陈继志1,2(),刘军2 |
2 洛阳船舶材料研究所, 洛阳 471000 |
|
STUDY ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 1000 MPa GRADE 0Cr16Ni5Mo STEEL |
Yongwei SUN1,Jizhi CHEN1,2(),Jun LIU2 |
1 College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001 2 Luoyang Ship Material Research Institute, Luoyang 471000 |
引用本文:
孙永伟,陈继志,刘军. 1000 MPa级0Cr16Ni5Mo钢的氢脆敏感性研究*[J]. 金属学报, 2015, 51(11): 1315-1324.
Yongwei SUN,
Jizhi CHEN,
Jun LIU.
STUDY ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 1000 MPa GRADE 0Cr16Ni5Mo STEEL[J]. Acta Metall Sin, 2015, 51(11): 1315-1324.
[1] | Kuduzovi? A, Poletti M C, Sommitsch C, Domankova M, Mitsche S, Kienreich R. Mater Sci Eng, 2014; A590: 66 | [2] | Tian Y, Wang M Q, Li J X, Shi J, Hui W J, Dong H. Acta Metall Sin, 2008; 44: 403 (田 野, 王毛球, 李金许, 时 捷, 惠卫军, 董 瀚. 金属学报, 2008; 44: 403) | [3] | Li H L, Hui W J, Wang Y B, Dong H, Weng Y Q, Chu W Y. Acta Metall Sin, 2001; 37: 512 (李会录, 惠卫军, 王燕斌, 董 瀚, 翁宇庆, 褚武扬. 金属学报, 2001; 37: 512) | [4] | Xiao J M. Acta Metall Sin, 1997; 33: 113 (肖纪美. 金属学报, 1997; 33: 113) | [5] | Chu W Y,Qiao L J,Li J X,Su Y J,Yan Y,Bai Y,Ren X C,Huang H Y. Hydrogen Embrittlement and Stress Corrosion Cracking. Beijing: Science Press, 2013: 557 (褚武扬,乔利杰,李金许,宿彦京,岩 雨,白 洋,任学冲,黄海友. 氢脆和应力腐蚀. 北京: 科学出版社, 2013: 557) | [6] | Hui W J,Weng Y Q,Dong H. The Steels of High-Strength Fasteners. Beijing: Metallurgical Industry Press, 2009: 64 (惠卫军,翁宇庆,董 瀚. 高强度紧固件用钢. 北京: 冶金工业出版社, 2009: 64) | [7] | Ham J, Jang Y, Lee G, Kim B, Rhee K, Cho C. Mater Sci Eng, 2013; A581: 83 | [8] | Fransplass H, Langseth M, Hopperstad O S. Int J Mechani Sci, 2011; 53: 946 | [9] | Chu W Y, Li J X, Huang Z H. Corrosion, 1999; 55: 892 | [10] | Troiano A R. Trans ASM, 1960; 52: 54 | [11] | Oriani R A. Acta Metall, 1970; 18: 147 | [12] | Thomans D. Acta Metall Mater, 1994; 42: 2043 | [13] | Birnbaum H K, Sofronis P. Mater Sci Eng, 1994; A176: 191 | [14] | Yokota T, Shiraga T. ISIJ Int, 2003; 43: 534 | [15] | Kissinger H E. Anal Chem, 1982; 29: 135 | [16] | Gu J L, Chang K D, Fang H S, Bai B Z. ISIJ Int, 2002; 42: 1560 | [17] | Pressouyre G M. Metall Trans, 1979; 10A: 1571 | [18] | Escobar D P, Verbeken K, Duprez L. Mater Sci Eng, 2012; A551: 50 | [19] | Hirth J P. Metall Trans, 1980; 11A: 861 | [20] | Sofronis P, Birnbaum H K. J Mech Phys Solids, 1995; 43: 49 | [21] | Nabarro F R N. Proc Roy Soc, 1940; 175A: 519 | [22] | Li J C M, Oriani R A, Darken L S. Z Physik Chem Neue Folge, 1966; 49: 271 | [23] | Sofronis P, McMeeking R M. J Mech Phys Solids, 1989; 37: 317 | [24] | Chateau J P, Delafosse D, Magnin T. Acta Mater, 2002; 50: 1507 | [25] | Eshelby J D. Proc Roy Soc, 1957; 241A: 376 | [26] | Li H L, Chu W Y, Gao K W, Qiao L J. Acta Metall Sin, 2002; 38: 849 (李会录, 褚武扬, 高克玮, 乔利杰. 金属学报, 2002; 38: 849) | [27] | Hardie D, Liu S E. Corros Sci, 1996; 38: 721 | [28] | Nagao A, Smith C D, Dadfarnia M, Sofronis P, Robertson I M. Proce Mater Sci, 2014; 3: 1700 | [29] | Robertson I M. Eng Fract Mech, 1999; 64: 649 | [30] | Abhay K J, Narayanan P R, Sreekumar K, Mittal M C, Ninan K N. Eng Fail Analy, 2008; 15: 431 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|