| PREPARATION OF NANOCRYSTALLINE TITANIA |
| GAO Rongjie;SHI Kexin;WANG Zhichang(Northeastern University;Shenyang 110006) SHEN Tongde(State Key Laboratory for RSA;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Department of Cheinistry;Northeastern University;Shenyang 110006)(Manuscript 1996-04-22) |
|
Cite this article:
GAO Rongjie;SHI Kexin;WANG Zhichang(Northeastern University;Shenyang 110006) SHEN Tongde(State Key Laboratory for RSA;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Department of Cheinistry;Northeastern University;Shenyang 110006)(Manuscript 1996-04-22). PREPARATION OF NANOCRYSTALLINE TITANIA. Acta Metall Sin, 1996, 32(10): 1097-1101.
|
|
|
Abstract Nanocrystalline titania particles were prepared by using precursor method from titanium tetrachloride.The microstructure was determined by using DTA-TG,XRD,TEM and Q-900 analyses.The results show that the spherical nanocrystal with rutile structure has an avarage diameter of 8.5 nm,good dispersity and purity.It's size distribution is from 5.0 nm to 15.0 nm.
|
|
Received: 18 October 1996
|
| 1EgonM.JColloidInterfaceSci,1977;61:3022MarioV.JColloidInterfaceSci,1979;68:3083LivageJ.MaterResSocSympProc,1986;73:7174姚光辉,李春忠,胡黎明.华东化工学院学报,1990,18:4495MorookaS,YesutakeT.IntChemEng,1989;29:1196罗菊,丁星兆.程黎放.材料科学进展,1993,7:527LawrenceHE,AndreasMG.JAmCeramSoc,1988;71:2258ChateBB.AmCeramBull,1973;52:6709KanerRB,BonneauPR,GillanEG,WileyJB,JarvisRF,TreeceREJr.USPat,5110768,199210HectorA,ParkinIP.JChemSocChemCommun,1993:109511HectorA,ParkinIP.Ployhedron,1993;12.109512WilliamFM.PowderDiffractionFile,AlphabeticalIndex(InorganicMaterial).Swarthmore:JCPDS,1982:84413GuinierA.X-rayDiffraction.SanFrancisco:Freeman,1963:124 |
| No Suggested Reading articles found! |
|
|