INFLUENCES OF Y~+-IMPLANTATION ON GROWTH STRESS OF OXIDE SCALE FORMED ON ALUMINIZED Ni-BASE ALLOY
XIN Li; LI Meishuan; LI Tiefan (Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

XIN Li; LI Meishuan; LI Tiefan (Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 110015). INFLUENCES OF Y~+-IMPLANTATION ON GROWTH STRESS OF OXIDE SCALE FORMED ON ALUMINIZED Ni-BASE ALLOY. Acta Metall Sin, 1996, 32(9): 949-954.

Download:  PDF(448KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influences of implanted yttrium with doses of 1×10~(17), 1×10~(16)Y~+/cm~2 on the growth stress of oxide scales formed on aluminized Ni-15Cr-6Al alloy were studied by using apparatus of oxide scale stress measurement. The experimental results indicated that Y~+-implantation at the two doses had no effects on the oxidation kinetics of the alloy, but decreased the growth stress in the oxide scale formed at 1100℃. The results are discussed. The reason that ion implantation with two doses decreases the growth stress and improves the adhension of alumina scale may be that Y~+- implantation changes the oxidation mechanism of the scale and facilitates the plastic deformation of the scale.
Key words:  oxidation      growth stress      Y~+-implantation      aluminized Ni-based alloy     
Received:  18 September 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I9/949

1ChoquetP,MevrelR.MaterSciEng,1989;A120:1532JedlinskiJ.In:LangEed.,TheRoleofActiveElementsintheOxidationBehaviourofHikhTemperatureMetalsandAlloys,London:ElsevierScience,1989:1313DelauneyD,HuntzAM.JMaterSci,1982;17:20274彭晓,李铁藩,李美栓,马信清,陈全芳.周龙江中国稀土学报,1994,(12):3285李铁藩,李美栓.金属学报,1992;28:B2096LiMeishuan,LiTiefan.MaterSciTechnol,1993;9:677李铁藩,曲英哲.理化检验(物理分册),1986;22:68范玉殿主编.电子束和离子束加工.北京:机械工业出版社,1989:2999AshworthV,GrantWA,ProcterRPM.CorrosSci,1976;6:66110工程材料实用手册编辑委员会.工程材料实用手册,北京:中国标准出版社,1989;2:68111JedlinskiJ,GodlewskiK,MrowecS.MaterSciEng,1989;A121:53912SmialekJL,GibalaR.MetallTrans,1983;14A:214313RybickiGC,SmialekJL.OxidMet.1989;31:27514SchumamE.OxidMet,1995;43:15715FintBA,HobbsW.JElectrochemSoc,1994;141:244316辛丽,李美栓,李铁藩.中国腐蚀与防护学报,1996;16;4217SamsonovGV.TheOxideHandbook.NewYork:IFI//Plenum,1982:1918DelauneyD,HuntzAM,LacombeP.CorrosSic,1980;20:110919RamanarayananTA,RaghavanM,PetkviclutonR.JElectrochemSoc,1984,131:92320JedlinskiJ,BorchardtD.OxidMet.1991;36:317
[1] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[2] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[3] LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature[J]. 金属学报, 2023, 59(3): 387-398.
[4] LI Xin, JIANG He, YAO Zhihao, DONG Jianxin. Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr[J]. 金属学报, 2023, 59(2): 309-318.
[5] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[6] JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui. Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing[J]. 金属学报, 2023, 59(10): 1324-1334.
[7] HU Min, ZHOU Shengyu, GUO Jingyuan, HU Minghao, LI Chong, LI Huijun, WANG Zumin, LIU Yongchang. Oxidation Behavior of Micro-Regions in Multiphase Ni3Al-Based Superalloys[J]. 金属学报, 2023, 59(10): 1346-1354.
[8] CONG Hongda, WANG Jinlong, WANG Cheng, NING Shen, GAO Ruoheng, DU Yao, CHEN Minghui, ZHU Shenglong, WANG Fuhui. A New Design Inorganic Silicate Composite Coating and Its Oxidation Behavior at High Temperature in Steam Atmosphere[J]. 金属学报, 2022, 58(8): 1083-1092.
[9] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[10] ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie. Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings[J]. 金属学报, 2022, 58(4): 503-512.
[11] SU Kaixin, ZHANG Jiwang, ZHANG Yanbin, YAN Tao, LI Hang, JI Dongdong. High-Cycle Fatigue Properties and Residual Stress Relaxation Mechanism of Micro-Arc Oxidation 6082-T6 Aluminum Alloy[J]. 金属学报, 2022, 58(3): 334-344.
[12] PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li. Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet[J]. 金属学报, 2022, 58(12): 1600-1610.
[13] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[14] CHEN Shenghu, RONG Lijian. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. 金属学报, 2021, 57(8): 989-999.
[15] PI Huilong, SHI Xiaolei, XU Xingxiang. Effect of SiC-ZrC Coating Prepared by SiZr Liquid Phase Sintering on the Oxidation Resistance of C/SiC Composites[J]. 金属学报, 2021, 57(6): 791-796.
No Suggested Reading articles found!