Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (9): 943-948    DOI:
Current Issue | Archive | Adv Search |
A MODEL WITH QUANTIFIED ASYMMETRY FOR PREDICTING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM
SHEN Jianyun; HAO Yaowu; ZHOU Chuanhua; LING Ling (General Research Institule for Non-Ferrous Metals; Beijing 100088)
Cite this article: 

SHEN Jianyun; HAO Yaowu; ZHOU Chuanhua; LING Ling (General Research Institule for Non-Ferrous Metals; Beijing 100088). A MODEL WITH QUANTIFIED ASYMMETRY FOR PREDICTING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM. Acta Metall Sin, 1996, 32(9): 943-948.

Download:  PDF(358KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new geometric model for predicting ternary thermodynamic properties from binaries is suggested. The model quantifies the asymmetric degree of the system with an exponent weight function according to the thermodynamic criterion, so as to avoid human interferences of choosing asymmetric component. It compares the similarity between every pair of binaries point by point, so that it can be applied to the system where the binary models do not cover the whole domains of compositions.
Key words:  thermodynamic model      ternary system      excess Gibbs free energy     
Received:  18 September 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I9/943

1KohlerF,Monat.FuerChemie,1960;91:7382MuggianuYM,GambinoM,BrosJP.ChemPhys,1975;22:833ToopGM.TransAIME,1965;233:8504ChouGC.CALPHAD,1994;24:385ChouGC.CALPHAD,1995;25:646QiaoZY,XingXR,ZhengCQ,DuanSZ.JRareEarths,1991;9:1817周传华.北京有色金属研究总院博士学位论文,19958LukasHL,HeingET,ZimmermannB.CALPHAD,1977;1:2259SaboungiML,LinPL,CerisierP,PeltonAD.MetallTrans,1980;11B:493
[1] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[2] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[3] Lü Baochen LIU Haitao REN Xin WANG Xiaoliang LI Gang SUN Yuejun. AN ATOM DENSE PACKING MODEL FOR METALLIC GLASS WITH HIGH SOLUTE CONCENTRATION IN (PSEUDO–) TERNARY SYSTEMS[J]. 金属学报, 2012, 48(2): 240-244.
[4] . A Model for Calculating Solubility of Hydrogen in Molten Alloys[J]. 金属学报, 2008, 44(2): 129-133 .
[5] . Quasicrystals in Al-Cu-Ni-Fe Quaternary System[J]. 金属学报, 2007, 43(4): 374-378 .
[6] ZHANG Xiaobing. Thermodynamic Modeling for Controls of Deoxidation and Oxide Inclusions in Molten Steel[J]. 金属学报, 2004, 40(5): 509-514 .
[7] LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn. STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM[J]. 金属学报, 1998, 34(9): 897-902.
[8] XU Kuangdi;JIANG Guochang; ZHANG Xiaobing; TANG Kai; XU Jianlun; DING Weizhong (Shanghai Enhaned Laboratory of Ferrometallurgy; Shanghai University; Shanghai 200072). THE NEW DEVELOPMENT OF THE SELF-SReM4 MODEL AND ITS APPLICATION TO THE QUARTERNARY SYSTEM OF C-Mn-Fe-Si[J]. 金属学报, 1998, 34(5): 459-466.
[9] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[10] LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM[J]. 金属学报, 1996, 32(11): 1171-1176.
[11] CHE Guangcan Institute of Physics; Academia Sinica; Beijing; ELLNER M. Max-Planck-Institut for Metallforschung; Stuttgart; Germany. PHASE DIAGRAM OF Bi-Pb-Tl TERNARY SYSTEM[J]. 金属学报, 1991, 27(6): 152-154.
[12] ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming. ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM[J]. 金属学报, 1991, 27(3): 147-149.
[13] CHEN Rongzhen;ZHANG Hanxing;ZHENG Jianxuan;HE Hanping Guangxi University; Nanning Guangxi Institute of Non-Ferrous Metals Geology; Nanning CHEN Rongzhen;Department of Physics;Guangxi University; Nanning;530009 Guangxi. 410℃ ISOTHERMAL SECTION OF Al-Cu-Sb TERNARY SYSTEM PHASE DIAGRAM[J]. 金属学报, 1989, 25(5): 142-143.
[14] ZHANG Kanghou;CHEN Lili Kunming Institute of Precious Metals ZHANG Kanghou; Kunming Institute of Precious Metals; 650221 Kunming. ROOM TEMPERATURE AND 750℃ ISOTHERMAL SECTIONS OF Ag-Pd-Gd TERNARY SYSTEM (Gd≤25 at.-%) PHASE DIAGRAM[J]. 金属学报, 1989, 25(5): 139-141.
[15] ZHENG Chaogui;JIN Jun;YE Yupu Peking University. LIQUIDUS OF NdCl_3-MgCl_2-LiCl SYSTEM[J]. 金属学报, 1989, 25(1): 147-149.
No Suggested Reading articles found!