| LASER REMELTED Ni-Cr-B-Si COATING ON Al-Si ALLOY |
| LIANG Gongying; LI Chenglao; SU Junyi (Xi'an Jiaotong University; Xi'an 710049) |
|
Cite this article:
LIANG Gongying; LI Chenglao; SU Junyi (Xi'an Jiaotong University; Xi'an 710049). LASER REMELTED Ni-Cr-B-Si COATING ON Al-Si ALLOY. Acta Metall Sin, 1997, 33(3): 315-319.
|
|
|
Abstract The plasma sprayed coating zone (Ni-Cr-B-Si) on an Al-Si alloy surface was remelted by a 5 kW CO2 laser. SEM and TEM analysis showed that there is crystalline and amorphous coexistent region. As the annealing effects caused by heat transfer of following melt and latent heat of crystallizing, some Ni3Al nano-crystallites (2-5 nm) formed and some of them grew gradually into globular grains (0. 1-0.2μm). The hardness in amorphous region is up to HV 1235 which is 3 times as high as that of plasma sprayed coating zone.
|
|
Received: 18 March 1997
|
1 El Mehairy A E. J Mater Sci, 1991; 26. 517 2 Pantelis D, Michaud H, De Freitas M. Surf Coat Technol, 1993; 57: 123 3 Escudero M L, Bello J M. Mater Sci Eng, 1992; A 158: 227 4 Yellup J M. Surf Coat Technol, 1995; 71: 121 5 Pierantoni M, Wagniere J D, Blank E. Mater Sci Eng, 1989; A110: L17 6 Pierantoni M, Gremaud M, Magnin P, Stoll D, Kurz W. Acta Metall Mater, 1992; 40:1637 7 Ohmori A, Kamada K. Trans JWRI,1991; 20(1): 137 8 Das D K. Surf Coat Technol, 1994, 64.11 9 Knotek O, Loffier F. Mater Sci Eng, 1991; A 140: 655 10 West D R F. Ternary Equdterium Diagrams. London: Chapman and Hall Ltd, 1982: 107 11 Smithells C J. Metals Reference Book. London: Fulmer Research Institute Ltd, 1976: 100, 399 12 Massalski T B Binary Alloy Diagrams.Metals Park,Ohio:ASM,1987:842,1086,1756 13 Wang H M,Zhang J H,Tang Y J,Hu Z Q,Yukawa N,Morinaga M,Murata Y.Mater Sci Eng,1992; A156:109 14 Babushkin V B,Voroshnin L G,Parkhimovich V V.Steel USSR,1990;20:511 15 Gremaud M,Carrard M,Kurz W.Acta Metall Mater,1990;38:2587 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|