LASER REMELTED Ni-Cr-B-Si COATING ON Al-Si ALLOY
LIANG Gongying; LI Chenglao; SU Junyi (Xi'an Jiaotong University; Xi'an 710049)
Cite this article: 

LIANG Gongying; LI Chenglao; SU Junyi (Xi'an Jiaotong University; Xi'an 710049). LASER REMELTED Ni-Cr-B-Si COATING ON Al-Si ALLOY. Acta Metall Sin, 1997, 33(3): 315-319.

Download:  PDF(1692KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The plasma sprayed coating zone (Ni-Cr-B-Si) on an Al-Si alloy surface was remelted by a 5 kW CO2 laser. SEM and TEM analysis showed that there is crystalline and amorphous coexistent region. As the annealing effects caused by heat transfer of following melt and latent heat of crystallizing, some Ni3Al nano-crystallites (2-5 nm) formed and some of them grew gradually into globular grains (0. 1-0.2μm). The hardness in amorphous region is up to HV 1235 which is 3 times as high as that of plasma sprayed coating zone.
Key words:  laser surface melting      aluminium alloy      amorphous      nanocrystal     
Received:  18 March 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I3/315

1 El Mehairy A E. J Mater Sci, 1991; 26. 517
2 Pantelis D, Michaud H, De Freitas M. Surf Coat Technol, 1993; 57: 123
3 Escudero M L, Bello J M. Mater Sci Eng, 1992; A 158: 227
4 Yellup J M. Surf Coat Technol, 1995; 71: 121
5 Pierantoni M, Wagniere J D, Blank E. Mater Sci Eng, 1989; A110: L17
6 Pierantoni M, Gremaud M, Magnin P, Stoll D, Kurz W. Acta Metall Mater, 1992; 40:1637
7 Ohmori A, Kamada K. Trans JWRI,1991; 20(1): 137
8 Das D K. Surf Coat Technol, 1994, 64.11
9 Knotek O, Loffier F. Mater Sci Eng, 1991; A 140: 655
10 West D R F. Ternary Equdterium Diagrams. London: Chapman and Hall Ltd, 1982: 107
11 Smithells C J. Metals Reference Book. London: Fulmer Research Institute Ltd, 1976: 100, 399
12 Massalski T B Binary Alloy Diagrams.Metals Park,Ohio:ASM,1987:842,1086,1756
13 Wang H M,Zhang J H,Tang Y J,Hu Z Q,Yukawa N,Morinaga M,Murata Y.Mater Sci Eng,1992; A156:109
14 Babushkin V B,Voroshnin L G,Parkhimovich V V.Steel USSR,1990;20:511
15 Gremaud M,Carrard M,Kurz W.Acta Metall Mater,1990;38:2587
[1] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[2] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[3] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[4] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[5] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[6] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[7] BI Jiazi, LIU Xiaobin, LI Ran, ZHANG Tao. Tribological Properties of Polyalphaolefin (PAO6) Lubricant Modified with Particles Additives of Metallic Glass[J]. 金属学报, 2021, 57(4): 559-566.
[8] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[9] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[10] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[11] LI Xiaoqian, WANG Fuguo, LIANG Aimin. Effect of Spraying Process on Microstructure and Tribological Properties of Ta2O5 In Situ Composite Nanocrystalline Ta-Based Coatings[J]. 金属学报, 2021, 57(2): 237-246.
[12] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[13] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[14] ZHAO Yanchun, MAO Xuejing, LI Wensheng, SUN Hao, LI Chunling, ZHAO Pengbiao, KOU Shengzhong, Liaw Peter K.. Microstructure and Corrosion Behavior of Fe-15Mn-5Si-14Cr-0.2C Amorphous Steel[J]. 金属学报, 2020, 56(5): 715-722.
[15] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
No Suggested Reading articles found!