| IN SITU OBSERVATION OF Z FORM PROPAGATION OF CRACKS IN 22Mn-13Cr-5Ni-0.2N STEEL |
| ZHANG Jingwu;LIU Wenchang;DUAN Zhixiang;ZHENG Yangreng (Yanshan University; Qinhuangdao 066004) |
|
Cite this article:
ZHANG Jingwu;LIU Wenchang;DUAN Zhixiang;ZHENG Yangreng (Yanshan University; Qinhuangdao 066004). IN SITU OBSERVATION OF Z FORM PROPAGATION OF CRACKS IN 22Mn-13Cr-5Ni-0.2N STEEL. Acta Metall Sin, 1997, 33(9): 927-932.
|
|
|
Abstract Z form propagation of cracks in 22Mn- 13Cr-5Ni-0.2N steel has been investigated by means of in situ tensile test in TEM. The results show that the Z form propagation of a crack in the steel is formed by the alternate progress of the relative sliding of the {111}and the cleavage along {100}, and is determined by the relative orientation between outside force and crystal.
|
|
Received: 18 September 1997
|
1Wilsdof H G F.Mater Sci Eng,1983;59:1 2Ohr S Mater Sci Eng, 1995;72:1 3陈明伟,林栋梁,梁伟.金属学报,1994 7:A331 4张静武,刘文昌,郑炀曾,赵红,管秀发,赵明德.兵器材料科学与工程,1993;5:40 5冯端,王业宁,丘第荣金属物理.北京:科学出版社,1975:639i |
| No Suggested Reading articles found! |
|
|