Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (9): 1002-1008    DOI:
Current Issue | Archive | Adv Search |
FABRICATION OF TiO_2 COATED C_f/ Al BY USING SOL-GEL TECHNIQUE
ZENG Qingbing(The First MedicaI University of PLA; Guangzhou 510515)
Cite this article: 

ZENG Qingbing(The First MedicaI University of PLA; Guangzhou 510515). FABRICATION OF TiO_2 COATED C_f/ Al BY USING SOL-GEL TECHNIQUE. Acta Metall Sin, 1997, 33(9): 1002-1008.

Download:  PDF(1366KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  TiO2 sol was prepared by hydrolysis and polycondensation of titania alkoxides in the presence of acetic acid. Further study focused on dipping TiO2 oxide coating on carbon fibers by sol-gel continous processing and fabrication of Cf/ Al preformed wire.Some characterization methods such as IR, TG-DTA, XRD, SEM are used. The results show that the effect of TiO2 coating depends on the viscosity of sol. After coating treatment,the cracks on carbon fiber surface are covered, oxidation resistance of carbon fibers is enhanced, the wettability between the fibers and melting aluminum is greatly improved and the tensile strength of C / Al prefabrication is heigtened.
Key words:  sol      gel      TiO_2      carbon fiber      coating      C/Al preformed wire     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/1002

1Jurek K,Guglielmi M,Kuncova G Renner O,Lukes F,Navratil M,Krousty E Vorlicek V,Kokesova K.J Mater Sci,1992;27:2549
2Helmer T,Peterlik H Kromp K J Am Ceram Soc,1995;1:133
3Von Thicle K H,Panse M.Z Anorg Allg Chem,1978;441:23
4Marrcus H L.AD-A127590, 1983
5Harding J, Welsh L M.J Mater Sci,1983;18:1810
6Huang S C,Hall E L,Gigliotti M F X.J Mater Res ,1988;3:1
7王尊德,刘宗荣,姚忠凯,姚枚.材料科学进展,1993;7:45
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[4] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[5] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[6] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[7] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[8] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[9] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[10] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[11] ZHANG Zhidong. Exact Solution of Ferromagnetic Three-Dimensional (3D) Ising Model and Spontaneous Emerge of Time[J]. 金属学报, 2023, 59(4): 489-501.
[12] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[13] WANG Di, HE Lili, WANG Dong, WANG Li, ZHANG Siqian, DONG Jiasheng, CHEN Lijia, ZHANG Jian. Influence of Pt-Al Coating on Tensile Properties of DD413 Alloy at High Temperatures[J]. 金属学报, 2023, 59(3): 424-434.
[14] LI Dou, XU Changjiang, LI Xuguang, LI Shuangming, ZHONG Hong. Thermoelectric Properties of P-Type CeyFe3CoSb12 Thermoelectric Materials and Coatings Doped with La[J]. 金属学报, 2023, 59(2): 237-247.
[15] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
No Suggested Reading articles found!