Abstract Al-30%Si alloy powder was prepared by high-pressure water atomization, and its oxygen content, particle size, morphology and microstructure were studied. Results show that the water atomization process can prepare fine particle size, even size distribution, low oxygen content powder. Due to rapid solidification, the silicon phases were greatly fined and the base-phase was reinforced, as compared with Al-30%Si cast alloy.
|
Received: 18 January 1998
|
1 Zhou J, Duszczyk J.J Mater Sci 1990; 25:4541 2 Zhou J,Duszczyk J, Korevaar B M.J Mater Sci,1991;26:3041 3 唐华生.金属材料研究,1991;17(1):45(Tang Huasheng.Res Metall Mater,1991; 17(1):45) 4 邱光汉,中南工业大学学报,1995; 25:484(Qiu Guanghan.J Cent South Uni Technol,1995;25:484) 5 李月珠。快速凝固技术和材料.北京:国防工业出版社,1993:122(Li Yuezh.Rapidly Solidified Technology and Material.Beijing:National defense Industry Press,1993:122)% |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|