Acta Metall Sin  1998, Vol. 34 Issue (1): 95-99    DOI:
Current Issue | Archive | Adv Search |
PROPERTIES OF A HIGH SILICON ALUMINIUM ALLOY POWDER PREMRED BY HIGH PRESSURE WATER ATOMIZATION
LI Yuanyuan; ZHANG Datong; XIA Wei;ZHANG Wen; WEN Liping (Mechanical and Electronic Engineering Department; South China University of Technology; Guangzhou 510641)
Cite this article: 

LI Yuanyuan; ZHANG Datong; XIA Wei;ZHANG Wen; WEN Liping (Mechanical and Electronic Engineering Department; South China University of Technology; Guangzhou 510641). PROPERTIES OF A HIGH SILICON ALUMINIUM ALLOY POWDER PREMRED BY HIGH PRESSURE WATER ATOMIZATION. Acta Metall Sin, 1998, 34(1): 95-99.

Download:  PDF(1858KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Al-30%Si alloy powder was prepared by high-pressure water atomization, and its oxygen content, particle size, morphology and microstructure were studied. Results show that the water atomization process can prepare fine particle size, even size distribution, low oxygen content powder. Due to rapid solidification, the silicon phases were greatly fined and the base-phase was reinforced, as compared with Al-30%Si cast alloy.
Key words:  high-pressure water atomization      rapid solidification      high Si-Al alloy powder     
Received:  18 January 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I1/95

1 Zhou J, Duszczyk J.J Mater Sci 1990; 25:4541
2 Zhou J,Duszczyk J, Korevaar B M.J Mater Sci,1991;26:3041
3 唐华生.金属材料研究,1991;17(1):45(Tang Huasheng.Res Metall Mater,1991; 17(1):45)
4 邱光汉,中南工业大学学报,1995; 25:484(Qiu Guanghan.J Cent South Uni Technol,1995;25:484)
5 李月珠。快速凝固技术和材料.北京:国防工业出版社,1993:122(Li Yuezh.Rapidly Solidified Technology and Material.Beijing:National defense Industry Press,1993:122)%
[1] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[2] Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG. Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. 金属学报, 2018, 54(5): 824-830.
[3] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[4] Jinfu LI, Yaohe ZHOU. Remelting of Primary Solid in Rapid Solidification of Deeply Undercooled Alloy Melts[J]. 金属学报, 2018, 54(5): 627-636.
[5] Qianqian GU, Ying RUAN, Haizhe ZHU, Na YAN. Influence of Cooling Rate on Microstructural Formation of Melt-Spun Fe-Al-Nb Ternary Alloy[J]. 金属学报, 2017, 53(6): 641-647.
[6] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
[7] Lei ZHAO,Hongxiang JIANG,Tauseef AHMAD,Jiuzhou ZHAO. STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY[J]. 金属学报, 2015, 51(7): 883-888.
[8] CHEN Feng, SU Dexi, TONG Yunxiang, NIU Liqun,WANG Haibo, LI Li. MICROSTRUCTURE AND PHASE TRANSFORMATION OF Ni43Co7Mn41Sn9 HIGH TEMPERATURE SHAPE MEMORY ALLOY RIBBON[J]. 金属学报, 2013, 49(8): 976-980.
[9] CHEN Shu, ZHAO Jiuzhou. SOLIDIFICATION OF MONOTECTIC ALLOY UNDER LASER SURFACE TREATMENT CONDITIONS[J]. 金属学报, 2013, 49(5): 537-543.
[10] LI Shaoqiang, CHEN Zhiyong, WANG Zhihong, LIU Jianrong, WANG Qingjiang, . MICROSTRUCTURE STUDY OF A RAPID SOLIDIFICATION POWDER METALLURGY HIGH TEMPERATURE TITANIUM ALLOY[J]. 金属学报, 2013, 29(4): 464-474.
[11] SHENG Liyuan, ZHANG Wei, LAI Chen, GUO Jianting,XI Tingfei, YE Hengqiang. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LAVES PHASE STRENGTHENING NiAl BASE COMPOSITE FABRICATED BY RAPID SOLIDIFICATION[J]. 金属学报, 2013, 49(11): 1318-1324.
[12] MO Yunfei, LIU Rangsu, LIANG Yongchao, ZHENG Naichao, ZHOU Lili,TIAN Zean, PENG Ping. MOLECULAR DYNAMICS SIMULATION ON THE EVOLUTION OF MICROSTRUCTURES OF LIQUID ZnxAl100−x ALLOYS DURING RAPID SOLIDIFICATION[J]. 金属学报, 2012, 48(8): 907-914.
[13] ZHAO Lei ZHAO Jiuzhou. STUDY OF THE SOLIDIFICATION OF Ni-Ag MONOTECTIC ALLOY[J]. 金属学报, 2012, 48(11): 1381-1386.
[14] CAO Yongqing LIN Xin WANG Zhitai YANG Haiou HUANG Weidong. MICROSTRUCTURE EVOLUTION OF Ni-Sn EUTECTIC ALLOY IN LASER RAPID SOLIDIFICATION[J]. 金属学报, 2011, 47(5): 540-547.
[15] ZHOU Shengyin HU Rui JIANG Li LI Jinshan KOU Hongchao CHANG Hui ZHOU Lian. DENDRITE GROWTH IN SOLIDIFICATION OF UNDERCOOLED Co80Pd20 ALLOY[J]. 金属学报, 2011, 47(4): 391-396.
No Suggested Reading articles found!