MICROSTRUCTURE FEATURES IN DIRECTIONALLY SOLIDIFIED Ni_3Al ALLOY AFTER HIGH TEMPERATURE DEFORMATION
GU Yuefeng; LIN Dongliang; SHAN Aidang (The Public Laboratory of State Education Commission for High Temperature Materials and High Temperature Tests; Shanghai Jiaotong University; Shanghai 200030)(CHEN Jiaguang; HU Fan; CAO Hanqing (Shanghai Baoshan Institute of Iron and Steel; Shanghai 201900)
Cite this article:
GU Yuefeng; LIN Dongliang; SHAN Aidang (The Public Laboratory of State Education Commission for High Temperature Materials and High Temperature Tests; Shanghai Jiaotong University; Shanghai 200030)(CHEN Jiaguang; HU Fan; CAO Hanqing (Shanghai Baoshan Institute of Iron and Steel; Shanghai 201900). MICROSTRUCTURE FEATURES IN DIRECTIONALLY SOLIDIFIED Ni_3Al ALLOY AFTER HIGH TEMPERATURE DEFORMATION. Acta Metall Sin, 1998, 34(4): 351-355.
Abstract Optical microscopy, transmission electron microscopy and scanning electron microscopy were used to examine microstructure features of the directionally solidified Ni3Al alloy deformed under tension at high temperature. The results show that initial columnar grain boundaries have not obviously changed during the deformation under higher strain rate and there are no substructure within the columnar grains. When strain rate is lower, the initial columnar grain boundaries firstly change into sawtooth shape and then evolve into small grain belts with increasing strain during superplastic deformation. The average grain size in belt is about 15 mm containing both low angle grain boundaries and high angle grain boundaries. It is suggested thata continuous recovery and recrystallization process took place during superplastic deformation in DS Ni3Al alloy.
1 清木青,和泉修.日本金属学会志,1979;43:1190(Aoki K, Izumi O J Jpn Inst Met, 1979; 43: 1190) 2 Liu C T, White C L; Horton J A. Acta Metall, 1985; 33: 213 3谷月峰,林栋梁,单爱党,刘毅,刘震云.金属学报,1997; 33:325(Gu Yuefeng,Lin Dongliang (Lin T L),Shan Aidang, Liu Yi, Liu Zhenyun. Acta Metall Sin, 1997; 33:325) 4 谷月峰,林栋梁,单爱党、刘毅,叶伟.金属学报, 1996; 32: 1144 (Gu Yuefeng, Lin Dongliang(Lin T L), Shan Aidang, Liu Yi, Ye Wei. Acta Metall Sin, 1996; 32: 1144) 5谷月峰,刘 毅,林栋梁.郭建亭电子显微学报,1994;13:497(Gu Yuefeng,Liu Yi,Lin Dongliang(Lin T L),Guo Jianting.J Chin Electron Microscopy Soc, 19942 13:497) 6Gottstein G, Chang L, Yung H F. Mater Sci Technol, 1991; 7: 158 7Lin Dongliang(Lin T L); Shan A D, Li D Q Scr Metall Mater, 1994; 31: 1455 8Li D Q, Shan A D, Liu Y, Lin Dongliang(Lin T L). Scr Metall Mater, 1995; 33: 685