Acta Metall Sin  1998, Vol. 34 Issue (4): 400-405    DOI:
Current Issue | Archive | Adv Search |
THE INFLUENCE OF MISMATCH SPEED RATIO ON TEXTURE DEVELOPMENT IN CROSS SHEAR ROLLED 3% SILICON STEEL
LIU Gang (School of Materials and Metallurgy; Northeastern University; Shenyang 110006; School of Chemical Science and Engineering; Liaoning University; Shenyang 110036)QI Kemin; WANG Fu; WANG Gang; LIANG Zhide (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)
Cite this article: 

LIU Gang (School of Materials and Metallurgy; Northeastern University; Shenyang 110006; School of Chemical Science and Engineering; Liaoning University; Shenyang 110036)QI Kemin; WANG Fu; WANG Gang; LIANG Zhide (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). THE INFLUENCE OF MISMATCH SPEED RATIO ON TEXTURE DEVELOPMENT IN CROSS SHEAR ROLLED 3% SILICON STEEL. Acta Metall Sin, 1998, 34(4): 400-405.

Download:  PDF(568KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Commercial grain oriented silicon steel was cold rolled by cross shear rolling (CSR) with different mismatch speed ratios (MSR), followed by industry annealing. The effects of MSR on the texture development were analyzed. Experimental Results show that the MSRexerts little effect on the surface layers and the area near the higher speed roll, but more influenceon the middle section. With increasing the MSR, the texture configuration at the subsurface andthe middle section can be improved significantly. In this process the texture development exhibitsthe "inherence ", but does not influence the final results. The effect of secondary recrystallizationannealing in a CSR process is similar to that in conventional rolling process, i.e. Goss texture grows abnormally, and form the only texture component. Under different MSR being used, thefinal texture and the magnetic properties of samples are resemble, so the MSR can be selectedwithin a certain range.
Key words:  cross shear rolling      mismatch speed ratio      silicon steel      texture     
Received:  18 April 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I4/400

1 Liu G,Wang F,Zuo L,Qi K M,Liang Z D .Scr Mater (in print)
2 Liu G, Wang F; Qi K M, Liang Z D Proc 11th Int Conf on Textures of Materials, Xi’an, China, 1996: 315
3刘 刚,王福,齐克敏,刘桂兰,梁志德.金属学报,1997;33:364Liu G, Wang F, Qi K M, Liu G L, Lians Z D. Acta Metall Sin, 1997 33: 364)
4 Liang Z D, Xu J Z, Wang F Proc. 6th Int Conf on Textures of Materials. Tokyo: ISIJ, 1981: 1259
5梁志德,徐家桢,王 福.织构材料的三维取向分析术-ODF分析沈阳:东北工学院出版社,1986:151(Liang Z D,Xu J I,Wang F.Three Dimension Orientation Distribution Function of Texture Materials ODF Analysis, Shenyand:Northeastern University Publisher,1986;151)
6刘 刚,王 福,苏 雷,魏兴权. 东北大学学报,1997;16:614(Liu G, Wang F, Su L, Wei X Q, J Northeastern Uni, 1997; 16: 614)
7朱泉,魏大伟. 板材异步轧制理论与实际沈阳:东北工学院出版社,1984:29(Zhu Q,Wei D W.Cross Shear Rolling Theory and Practice of Sheets. Shenyang:Northeastern University Publisher, 1984; 29)
8 Cui D L,Shi J,Wang X J. Proc 11th Int Conf on Textures of Materials, Xi'an, China, 1996:717
9 Mishra S, Darmann C; Lu cke K. Acta Metall, 1984; 32(12): 2185
10 To th L S. Proc 11th Int Conf on Textures of Materials, Xi’an, China, 1996: 347
11王廷溥.金属塑性加工学. 北京:冶金工业出版社,1988:6 (Wang T F Plastic Forming of Metals. Beijing:The Metallurgical Industry Press,1988:6)
12 Koh P K, Dunn C G Trans AIME, 1955; 203: 401
13 Hu H.In:Himmel L ed .Recovery and Recrystallization of metals. New York: Interscience, 1964:311
14 Bottcher A, Hastenrath M, Lucke K Textures Microstruct, 1991; 14-18: 799
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[4] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
[5] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[6] YAN Mengqi, CHEN Liquan, YANG Ping, HUANG Lijun, TONG Jianbo, LI Huanfeng, GUO Pengda. Effect of Hot Deformation Parameters on the Evolution of Microstructure and Texture of β Phase in TC18 Titanium Alloy[J]. 金属学报, 2021, 57(7): 880-890.
[7] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[8] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.
[9] YU Lei,LUO Haiwen. Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel[J]. 金属学报, 2020, 56(3): 291-300.
[10] CHENG Chao,CHEN Zhiyong,QIN Xushan,LIU Jianrong,WANG Qingjiang. Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate[J]. 金属学报, 2020, 56(2): 193-202.
[11] DU Zijie, LI Wenyuan, LIU Jianrong, SUO Hongbo, WANG Qingjiang. Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process[J]. 金属学报, 2020, 56(12): 1667-1680.
[12] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
[13] Liping DENG,Kaixuan CUI,Bingshu WANG,Hongliang XIANG,Qiang LI. Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. 金属学报, 2019, 55(8): 976-986.
[14] Zheng LIU,Jianrong LIU,Zibo ZHAO,Lei WANG,Qingjiang WANG,Rui YANG. Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing[J]. 金属学报, 2019, 55(6): 692-700.
[15] Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN. Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. 金属学报, 2019, 55(5): 566-574.
No Suggested Reading articles found!