| INTERDIFFUSION IN LOW TEMPERATURE ANNEALED CoN/CN SOFT X-RAY MULTILAYER MIRRORS |
| BAI Haili; JIANG Enyong (Department of Applied Physics; Tianjin University; Tianjin 300072) |
|
Cite this article:
BAI Haili; JIANG Enyong (Department of Applied Physics; Tianjin University; Tianjin 300072). INTERDIFFUSION IN LOW TEMPERATURE ANNEALED CoN/CN SOFT X-RAY MULTILAYER MIRRORS. Acta Metall Sin, 1998, 34(4): 406-411.
|
|
|
Abstract The interdiffusion in the amorphous CoN/CN soft X-ray multilayer is investigated quantitatively by monitoring the enhancement of the first order modulation peak onannealing in the temperature range of 473-523 K. The effective interdiffusion coefficient measured is as low as 10-25m2s-1. The comparison with the results of Co/C system indicates that the following three features are noticeable: (1) the critical wavelengths of interdiffusion obtained are 2.00-2.04 nm at temperatures ranging from 473 to 523 K and equal to those of Co/C multilayers within the experimental error, indicating that the interdiffosion behaviour in the CoN/CNmultilayers still depends on the thermodynamic properties of the Co--C system, (2) the effectiveinterdffesivities and macroscopic diffusion coefficiellts are lower, and (3) the activation energy ofdiction is higher. The results imply that it is possible to improve the thermal stability of Co/Cmultilayer by doping with nitrogen.
|
|
Received: 18 April 1998
|
1 Bai H L, Jiang E Y, Wang C D. Thin Solid Filme, 1996; 286: 176 2 Greer A L, Spapan F. In: Chang L L, Giessen B C eds., Synthetic Modulation Structures. New York: Academic Press, 1985: 424 3 Jiang Xiaoming, Xian Dingchang, Wu Ziqin. Appl Phys Lett, 1990; 57: 2549 4 Sasanuma Y, Uchida M, Okada K, Yamamoto K, Kitano Y, Ishitani A. Thin Solid Films, 1991; 203: 113 5 Sasanuma Y, Nakayama K. Thin Solid Filme, 1994; 247: 24 6 Johansson B, Martensson N. Phys Rev, 1980; 21B: 4427 7 Steiner P, Hufner S, Martensson N, Johansson B. Solid State Commun, 1981; 37: 73 8 Miedema A R, de Chatel P F, de Boer F R. Physica, 1980; 100B: 1 9 Miedema A R. J Less-Common Met, 1976; 46: 67 10 Niessen A K, Miedema A R, de Beer F R, Boom R. Physica, 1988; 151B: 401+ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|