EFFECTS OF CONVECTIONS AND MOTIONS OF MINORITY PHASE DROPLETS ON SOLIDIFICATION OF MONOTECTIC ALLOYS
ZHAO Jiuzhou; LI Haili; ZHAO Lei
Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

ZHAO Jiuzhou LI Haili ZHAO Lei. EFFECTS OF CONVECTIONS AND MOTIONS OF MINORITY PHASE DROPLETS ON SOLIDIFICATION OF MONOTECTIC ALLOYS. Acta Metall Sin, 2009, 45(12): 1435-1440.

Download:  PDF(933KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Many alloys show a phase diagram characterized by the appearance of a miscibility gap in the liquid state. Some of them have great potentials to be used in industry. But when a homogeneous, single–phase liquid is cooled into the miscibility gap, the components are no longer miscible and two liquid phases develop. Generally the liquid–liquid decomposition causes the formation of the microstructure with serios segregation. The microstructure evolution during the liquid—liquid phase transformation of monotectic alloys is a result of the common actions of manfactors. It is very complex, especially the convection of the matrix and the motion of the minority phase droplets migt mix thigs p and make it extremely difficult to ivestigate te solidification process of monotectic alloys. In this paper, the effects of convection and minority phase droplet motion on the solidification of monotectic alloys were introducedthe current situation of researces in this field was overviewed.

Key words:  monotectic alloy      liquid-liquid phase transformation      convection      solidification      overview     
Received:  23 April 2009     
ZTFLH: 

TG113.12

 
Fund: 

Supported by National Natural Science Foundation of China (Nos.u0837601, 50771097 and 50671111)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I12/1435

[1] Zhao J Z. J Mater Sci Technol, 2002; 3: 197
[2] Liu Y, Guo J J, Jia J. Foundry, 2000; 49: 11
(刘源, 郭景杰, 贾均. 铸造, 2000; 49: 11)
[3] Zheng H X, Ma W Z, Guo X F. Rare Met Mater Eng, 2004; 33: 893
(郑红星, 马伟增, 郭学锋. 稀有金属材料与工程, 2004; 33: 893)
[4] Yang S, Huang W D. Mater Mech Eng, 2000; 24: 5
(杨森, 黄卫东. 机械工程材料, 2000; 24: 5)
[5] Zhao J Z, Ratke L. Z Metallkd, 1998; 89: 241
[6] Zhao J Z. Mater Sci Technol, 2001; 9: 154
(赵九洲. 材料科学与工艺, 2001; 9: 154)
[7] Zhao J Z, Hu Z Q. Acta Metall Sin, 2004; 40: 27
(赵九洲, 胡壮麒. 金属学报, 2004; 40: 27)
[8] Carlberg T, Fredriksson H. Metall Trans, 1982; 11A: 1665
[9] Granasy L, Ratke L. Scr Mater, 1993; 28: 1329
[10] Thieringer W K, Ratke L. Acta Metall, 1987; 35: 1237
[11] Heaby R B, Cahn J W. J Chen Phys, 1973; 58: 896
[12] Schaffer P L, Mathiesen R L, Arnberg L, Sabatino M D, Snigirev A. New J Phys, 2008; 10: 053001
[13] Li H L, Zhao J Z, Zhang Q X. Metall Mater Trans, 2008; 39A: 3308
[14] Zhao J Z. Mater Sci Eng, 2007; A454–455: 637
[15] Li H L, Zhao J Z, Li Z Y, He J. Acta Metall Sin, 2008; 44: 1081
(李海丽, 赵九洲, 李中原, 何杰. 金属学报, 2008; 44: 1081)
[16] Zhao J Z, Gao L L. Appl Phys Lett, 2005; 87: 131905
[17] Zhao J Z, Gao L L. J Mater Sci Technol, 2006; 22: 321
[18] Zhao J Z, Guo J J, Jia J. Trans Nonferrous Met Soc Chin, 1995; 5: 67
[19] Ratke L. In: Koster J N, Sani R L eds., Progress in Astronautics and Aeronautics, Vol.130, Washington, DC: AIAA, 1991: 661
[20] Ratke L, Thieringer W. Acta Metall, 1985; 33: 1793
[21] Zhao J Z, Guo J J, Jia J. Trans Nonferrous Met Soc China, 199; 5: 85
[22] Guo J J, Liu Y, Jia J, Su Y Q, Ding H S, Zhao J Z, Xue X. Scr Mater, 2001; 45: 1197
[23] Zhao J Z. PhD Thesis, Harbin Institute of Technology, 1994
(赵九洲. 哈尔滨工业大学博士学位论文, 1994)
[24] Gelles S H, Markworth A J. NASA TM78125, 1977
[25] Ratke L, Diefenbach S. Mater Sci Eng, 1995; R15: 263
[26] He J, Zhao J Z. Acta Metall Sin, 2006; 42: 67
(何杰, 赵九洲. 金属学报, 2006; 42: 67)
[27] Decarlo J L, Pirch R G. Metall Trans, 1984; 15A: 2155
[28] Foner S, Meniff E. Rev Sci Inst, 1968; 39: 171
[29] Zhang L, Wang E G, Zuo X W, He J C. Acta Metall Sin, 2008; 44: 165
(张林, 王恩刚, 左小伟, 赫冀成. 金属学报, 2008; 44: 165)
[30] Yasuda H, Ohnaka I, Fujimoto S. Mater Lett, 2004; 58: 911
[31] Yasuda H, Ohnaka I, Kawakami O. ISIJ Int, 2003; 43: 942
[32] Yasuda H, Ohnaka I, Fujimoto S. Scr Mater, 2006; 54: 527
[33] Zhao J Z, Jia J, Li Q C, Zhao Z M. Foundry, 1993; 8: 18
(赵九洲, 贾均, 李庆春, 赵忠民. 铸造, 1993; 8: 18)
[34] Jia J, Zhao J Z. Chin J Mech Eng, 1991; 4: 90
[35] Hao W X. Spec Cast & Nonferrous Alloys, 2004; 3: 22
(郝维新. 特种铸造及有色金属, 2004; 3: 22)
[36] Wang H P. Chin Sci Bull, 2004; 49: 322
[37] Ozawa S, Motegi T. Mater Lett, 2004; 58: 2548
[38] Cao C D, Wei B B. J Mater Sci Technol, 2002; 18: 73
[39] Li H L, Zhao J Z. Appl Phys Lett, 2008; 92: 241902
[40] Otto G, Frohbe G. In: 6th European Symposium on Materials Science Under Microgravity, Bordeaux, France: ESA–SP 256, 1987: 355
[41] Zhao J Z. Scr Mater, 2006; 54: 247
[42] Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K. Science, 2002; 297: 990
[43] Bradley E, Banerji K. IEEE Trans Components Packag Manuf Technol, 1996; B19: 320

[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[4] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[5] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[6] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[7] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[8] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[9] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[10] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[11] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[12] ZHANG Lei, SHI Tao, HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao. Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. 金属学报, 2022, 58(2): 225-230.
[13] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[14] CAO Jianghai, HOU Zibing, GUO Zhongao, GUO Dongwei, TANG Ping. Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet[J]. 金属学报, 2021, 57(5): 586-594.
[15] XU Junfeng, ZHANG Baodong, Peter K Galenko. Model of Eutectic Transformation Involving Intermetallic Compound[J]. 金属学报, 2021, 57(10): 1320-1332.
No Suggested Reading articles found!