| EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL |
| JIANG Huifeng1;2; CHEN Xuedong1;FAN Zhichao1;DONG Jie1;2;JIANG Heng1;LU Shouxiang2 |
1 National Technology Research Center on Pressure Vessel and Pipeline Safety Engineering; Hefei General Machinery Research Institute; Hefei 230031
2 Department of Safety Science and Engineering; University of Science and Technology of China; Hefei 230027 |
|
Cite this article:
JIANG Huifeng CHEN Xuedong FAN Zhichao DONG Jie JIANG Heng LU Shouxiang. EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL. Acta Metall Sin, 2009, 45(3): 326-330.
|
|
|
Abstract The fatigue--creep behaviors of hot rolled and dynamic strain aging pre--treated 316L austenitic stainless steels were investigated under different loading conditions at 550 ℃. Under stress control mode, the macroscopic manifestation of dynamic strain aging is the abrupt displacement jumps during cyclic deformation. By comparing with the hot rolled treatment the dynamic strain aging pre--treatment makes the cyclic strain amplitude decrease and the cycle number at the first abrupt displacement jump postpone, i.e., the material strength is enhanced and fatigue--creep life is effectively prolonged.
|
|
Received: 01 September 2008
|
|
|
| Fund: Supported by National Great Project of Scientific and Technical Supporting Program of China During the 11th Five--year Plan (No.2006BAK02B02--02) and Anhui Province Outstanding Youth Fund (No.08040106827) |
| [1] Plumbridge W J. J Mater Proc Technol, 1996; 56: 502
[2] Qian K W, Li X Q, Xiao L G. J Fuzhou Univ (Nat Sci), 2001; 29: 8
(钱匡武, 李孝琦, 萧林钢. 福州大学学报(自然科学版), 2001; 29: 8)
[3] Chen W Z, Qian K W. Acta Metall Sin, 1989; 25: 132
(陈文哲, 钱匡武. 金属学报, 1989; 25: 132)
[4] Peng K P, Chen W Z, Qian K W. Acta Metall Sin, 1993; 29: 283
(彭开萍, 陈文哲, 钱匡武. 金属学报, 1993; 29: 283)
[5] Jiang H F, Zhang Q C, Chen X D. Acta Mater, 2007; 55: 2219
[6] Jiang H F, Zhang Q C, Jiang Z Y, Wu X P. Acta Metall Sin, 2005; 41: 727
(江慧丰, 张青川, 蒋震宇, 伍小平. 金属学报, 2005; 41: 727)
[7] Jiang H F, Zhang Q C, Xu Y H, Wu X P. Acta Metall Sin, 2006; 42: 139
(江慧丰, 张青川, 徐毅豪, 伍小平. 金属学报, 2006; 42: 139)
[8] Hong S G, Lee S B, Byun T S. Mater Sci Eng, 2007; A457: 139
[9] Mannan S L. Bull Mater Sci, 1993; 16: 561
[10] Hong S G, Lee S B. J Nucl Mater, 2004; 328: 232
[11] Zhang L, Jiang H F, Jiang H. Pressure Vessel Technology, 2008; 25(7): 6
(张莉, 江慧丰, 姜恒. 压力容器, 2008; 25(7): 6)
[12] Miguel M C, Vespignani A, Zapperi S. Nature, 2001; 410: 667 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|