EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL
JIANG Huifeng1;2; CHEN Xuedong1;FAN Zhichao1;DONG Jie1;2;JIANG Heng1;LU Shouxiang2
1 National Technology Research Center on Pressure Vessel and Pipeline Safety Engineering; Hefei General Machinery Research Institute; Hefei 230031
2 Department of Safety Science and Engineering; University of Science and Technology of China; Hefei 230027
Cite this article: 

JIANG Huifeng CHEN Xuedong FAN Zhichao DONG Jie JIANG Heng LU Shouxiang. EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL. Acta Metall Sin, 2009, 45(3): 326-330.

Download:  PDF(803KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The fatigue--creep behaviors of hot rolled and dynamic strain aging pre--treated 316L austenitic stainless steels were investigated under different loading conditions at 550 ℃. Under stress control mode, the macroscopic manifestation of dynamic strain aging is the abrupt displacement jumps during cyclic deformation. By comparing with the hot rolled treatment the dynamic strain aging pre--treatment makes the cyclic strain amplitude decrease and the cycle number at the first abrupt displacement jump postpone, i.e., the material strength is enhanced and fatigue--creep life is effectively prolonged.

Key words:  316L stainless steel      fatigue-creep      dynamic strain aging      stress control      high temperature     
Received:  01 September 2008     
ZTFLH: 

O346.2

 
  TG142.71

 
Fund: 

Supported by National Great Project of Scientific and Technical Supporting Program of China During the 11th Five--year Plan (No.2006BAK02B02--02) and Anhui Province Outstanding Youth Fund (No.08040106827)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I3/326

[1] Plumbridge W J. J Mater Proc Technol, 1996; 56: 502
[2] Qian K W, Li X Q, Xiao L G. J Fuzhou Univ (Nat Sci), 2001; 29: 8
(钱匡武, 李孝琦, 萧林钢. 福州大学学报(自然科学版), 2001; 29: 8)

[3] Chen W Z, Qian K W. Acta Metall Sin, 1989; 25: 132
(陈文哲, 钱匡武. 金属学报, 1989; 25: 132)

[4] Peng K P, Chen W Z, Qian K W. Acta Metall Sin, 1993; 29: 283
(彭开萍, 陈文哲, 钱匡武. 金属学报, 1993; 29: 283)
[5] Jiang H F, Zhang Q C, Chen X D. Acta Mater, 2007; 55: 2219
[6] Jiang H F, Zhang Q C, Jiang Z Y, Wu X P. Acta Metall Sin, 2005; 41: 727
(江慧丰, 张青川, 蒋震宇, 伍小平. 金属学报, 2005; 41: 727)

[7] Jiang H F, Zhang Q C, Xu Y H, Wu X P. Acta Metall Sin, 2006; 42: 139
(江慧丰, 张青川, 徐毅豪, 伍小平. 金属学报, 2006; 42: 139)

[8] Hong S G, Lee S B, Byun T S. Mater Sci Eng, 2007; A457: 139
[9] Mannan S L. Bull Mater Sci, 1993; 16: 561
[10] Hong S G, Lee S B. J Nucl Mater, 2004; 328: 232
[11] Zhang L, Jiang H F, Jiang H. Pressure Vessel Technology, 2008; 25(7): 6
(张莉, 江慧丰, 姜恒. 压力容器, 2008; 25(7): 6)

[12] Miguel M C, Vespignani A, Zapperi S. Nature, 2001; 410: 667

[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[4] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[5] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[6] XU Jinghui, LI Longfei, LIU Xingang, LI Hui, FENG Qiang. Thermal-Stress Coupling Effect on Microstructure Evolution of a Fourth-Generation Nickel-Based Single-Crystal Superalloy at 1100oC[J]. 金属学报, 2021, 57(2): 205-214.
[7] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[8] YU Chenfan, ZHAO Congcong, ZHANG Zhefeng, LIU Wei. Tensile Properties of Selective Laser Melted 316L Stainless Steel[J]. 金属学报, 2020, 56(5): 683-692.
[9] LI Xiaohui, WANG Jianqiu, HAN En-Hou, GUO Yanjun, ZHENG Hui, YANG Shuangliang. Electrochemistry and In Situ Scratch Behavior of 690 Alloy in Simulated Nuclear Power High Temperature High Pressure Water[J]. 金属学报, 2020, 56(11): 1474-1484.
[10] BAO Feiyang, LI Yanfen, WANG Guangquan, ZHANG Jiarong, YAN Wei, SHI Quanqiang, SHAN Yiyin, YANG Ke, XU Bin, SONG Danrong, YAN Mingyu, WEI Xuedong. Corrosion Behaviors and Mechanisms of ODS Steel Exposed to Static Pb-Bi Eutectic at 600 and 700 ℃[J]. 金属学报, 2020, 56(10): 1366-1376.
[11] Jinyao MA,Jin WANG,Yunsong ZHAO,Jian ZHANG,Yuefei ZHANG,Jixue LI,Ze ZHANG. Investigation of In Situ 1150 ℃ High Temperature Deformation Behavior and Fracture Mechanism of a Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(8): 987-996.
[12] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[13] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[14] Dan LI, Yang LI, Rongsheng CHEN, Hongwei NI. Direct Synthesis of NiCo2O4 Nanoneedles and MoS2 Nanoflakes Grown on 316L Stainless Steel Meshes by Two Step Hydrothermal Method for HER[J]. 金属学报, 2018, 54(8): 1179-1186.
[15] Tingguang LIU, Shuang XIA, Qin BAI, Bangxin ZHOU. Morphological Characteristics and Size Distributions of Three-Dimensional Grains and Grain Boundaries in 316L Stainless Steel[J]. 金属学报, 2018, 54(6): 868-876.
No Suggested Reading articles found!