Solidification regularity of highly undercooled Fe-Co alloy |
;;;;; |
西北工业大学凝固技术国家重点实验室 |
|
Cite this article:
;. Solidification regularity of highly undercooled Fe-Co alloy. Acta Metall Sin, 2007, 43(5): 449-453 .
|
Abstract Fe-Co melts with different Co contents were undercooled using fluxing purification method. With increasing the initial melt undercooling, grain refinement occurs twice in Fe100-x-Cox(x=10-40) alloy, except Fe90Co10. While the microstructure is no longer single phase and metastable phase appears when undercooling of the melt exceeds the critical undercooling. Moreover, except transition at low undercooling, the exact undercooling for microstructure transition and the critical undercooling for forming of metastable phase increase with the content of Co. Furthermore, BCT model and transient nucleation theory were applied to analyze the microstructure evolutions of Fe-Co alloy.
|
Received: 07 September 2006
|
|
[1] Cech R E. Trans AIME, 1956; 206: 585 [2] Norman A F, Eckler K, Zambon A, Gartner F, Moir S A, Ramous E, Herlach D M, Greer A L. Ada Mater, 1998; 46: 3355 [3] Norman A F, Eckler K, Gartner F, Moir S A, Zambon A, Greer A L, Ramous E, Herlach D M. Mater Sci Eng, 1997; A226-228: 48 [4] Herlach D M, Feuerbacher B, Schleip E. Mater Sci Eng, 1991; A133: 795 [5] Eckler K, Gartner F, Assadi H, Norman A F, Greer A L, Herlach D M. Mater Sci Eng, 1997; A226-228: 410 [6] Norman A F, Hrtner G F, Greer A L. Mater Sci Form, 1996; 215-216: 21 [7] Herlach D M, Eckler K, Karma A, Schwarz M. Mater Sci Eng, 2001; A304-306: 20 [8] Han X J, Yang C, Wei B, Chen M, Guo Z Y. Mater Sci Eng, 2001; A307: 35 [9] Moir S A, Eckler K, Herlach D M. Acta Mater, 1998; 46: 4029 [10] Loser W, Herlach D M. Metall Trans, 1992; 23A: 1585 [11] Koseki T, Flemings M C. Metall Mater Trans, 1995; 26A: 2991 Koseki T, Flemings M C. Metall Mater Trans, 1996; 27A: 3226 Koseki T, Flemings M C. Metall Mater Trans, 1997; 28A: 1 [12] Liu N, Yang G C, Chen Y Z, Zhou Y H. Prog Nat Sci, 2006; 16: 120 (刘宁,杨根仓,陈豫增,周尧和.自然科学进展,2006;16: 120) [13] Liu N, Yang G C, Liu F, Chen Y Z, Yang C L, Zhou Y H. Mater Charact, 2006; 57: 115 [14] Liu N, Liu F, Yang G C, Chen Y Z, Yang C L, Zhou Y H. Physica, 2007; 387B: 151 [15] Hermann R, Loser W, Lindenkreuz G, Diefenbach A, Zah- now W, Dreier W, Volkmann T, Herlach D M. Mater Sci Eng, 2004; A375-377: 507 [16] Guo X F, Yang G C. Chin J Nonferrous Met, 2000; 10: 77 (郭学锋,杨根仓.中国有色金属学报, 2000;10:77) [17] Lipton J, Kurz W, Trivedi R. Acta Metall, 1987; 35: 957 [18] Lipton J, Kurz W, Trivedi R. Acta Metall, 1987; 35: 965 [19] Boettinger W J, Coriell S R, Trivedi R. In: Mehrabian R, Parrish P A, eds., Proc 4th Conf on Rapid Solidification Processing: Principles and Technologies, Baton Rouge, LA: Claitor's, Publishing Dirosion, 1988: 13 [20] Karma A. Int J Non-Equil Process, 1998; 11: 201 [21] Shao G, Tsakiropoulos P. Acta Metall Mater, 1994; 42: 2937 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|