Solidification regularity of highly undercooled Fe-Co alloy
;;;;;
西北工业大学凝固技术国家重点实验室
Cite this article: 

;. Solidification regularity of highly undercooled Fe-Co alloy. Acta Metall Sin, 2007, 43(5): 449-453 .

Download:  PDF(387KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fe-Co melts with different Co contents were undercooled using fluxing purification method. With increasing the initial melt undercooling, grain refinement occurs twice in Fe100-x-Cox(x=10-40) alloy, except Fe90Co10. While the microstructure is no longer single phase and metastable phase appears when undercooling of the melt exceeds the critical undercooling. Moreover, except transition at low undercooling, the exact undercooling for microstructure transition and the critical undercooling for forming of metastable phase increase with the content of Co. Furthermore, BCT model and transient nucleation theory were applied to analyze the microstructure evolutions of Fe-Co alloy.
Key words:  Fe-Co lloy      solidification      high undercooling      
Received:  07 September 2006     
ZTFLH:  TG113.1  
  TG146.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I5/449

[1] Cech R E. Trans AIME, 1956; 206: 585
[2] Norman A F, Eckler K, Zambon A, Gartner F, Moir S A, Ramous E, Herlach D M, Greer A L. Ada Mater, 1998; 46: 3355
[3] Norman A F, Eckler K, Gartner F, Moir S A, Zambon A, Greer A L, Ramous E, Herlach D M. Mater Sci Eng, 1997; A226-228: 48
[4] Herlach D M, Feuerbacher B, Schleip E. Mater Sci Eng, 1991; A133: 795
[5] Eckler K, Gartner F, Assadi H, Norman A F, Greer A L, Herlach D M. Mater Sci Eng, 1997; A226-228: 410
[6] Norman A F, Hrtner G F, Greer A L. Mater Sci Form, 1996; 215-216: 21
[7] Herlach D M, Eckler K, Karma A, Schwarz M. Mater Sci Eng, 2001; A304-306: 20
[8] Han X J, Yang C, Wei B, Chen M, Guo Z Y. Mater Sci Eng, 2001; A307: 35
[9] Moir S A, Eckler K, Herlach D M. Acta Mater, 1998; 46: 4029
[10] Loser W, Herlach D M. Metall Trans, 1992; 23A: 1585
[11] Koseki T, Flemings M C. Metall Mater Trans, 1995; 26A: 2991 Koseki T, Flemings M C. Metall Mater Trans, 1996; 27A: 3226 Koseki T, Flemings M C. Metall Mater Trans, 1997; 28A: 1
[12] Liu N, Yang G C, Chen Y Z, Zhou Y H. Prog Nat Sci, 2006; 16: 120 (刘宁,杨根仓,陈豫增,周尧和.自然科学进展,2006;16: 120)
[13] Liu N, Yang G C, Liu F, Chen Y Z, Yang C L, Zhou Y H. Mater Charact, 2006; 57: 115
[14] Liu N, Liu F, Yang G C, Chen Y Z, Yang C L, Zhou Y H. Physica, 2007; 387B: 151
[15] Hermann R, Loser W, Lindenkreuz G, Diefenbach A, Zah- now W, Dreier W, Volkmann T, Herlach D M. Mater Sci Eng, 2004; A375-377: 507
[16] Guo X F, Yang G C. Chin J Nonferrous Met, 2000; 10: 77 (郭学锋,杨根仓.中国有色金属学报, 2000;10:77)
[17] Lipton J, Kurz W, Trivedi R. Acta Metall, 1987; 35: 957
[18] Lipton J, Kurz W, Trivedi R. Acta Metall, 1987; 35: 965
[19] Boettinger W J, Coriell S R, Trivedi R. In: Mehrabian R, Parrish P A, eds., Proc 4th Conf on Rapid Solidification Processing: Principles and Technologies, Baton Rouge, LA: Claitor's, Publishing Dirosion, 1988: 13
[20] Karma A. Int J Non-Equil Process, 1998; 11: 201
[21] Shao G, Tsakiropoulos P. Acta Metall Mater, 1994; 42: 2937
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[4] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[5] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[6] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[7] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[8] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[9] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[10] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[11] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[12] ZHANG Lei, SHI Tao, HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao. Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. 金属学报, 2022, 58(2): 225-230.
[13] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[14] CAO Jianghai, HOU Zibing, GUO Zhongao, GUO Dongwei, TANG Ping. Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet[J]. 金属学报, 2021, 57(5): 586-594.
[15] ZHANG Zhuang, LI Haiyang, ZHOU Lei, LIU Huasong, TANG Haiyan, ZHANG Jiaquan. As-Cast Spot Segregation of Gear Steel and Its Evolution in the Rolled Products[J]. 金属学报, 2021, 57(10): 1281-1290.
No Suggested Reading articles found!