Abstract  The grain boundary character distributions (GBCD) of Pb-0.05%Ca-1.5%Sn-0.026%Al (mass fraction)alloy, which was solution treated at 290℃ and solution treated followed by pre-ageing at 100℃~200℃ prior to the same strain annealing, were investigated by means of electron back scatter diffraction ( EBSD) techniques. The results indicate that special boundaries were largely populated in the specimen which was strain annealed just after solution treatment. The fractions of ∑3 and(∑9+∑27)boundaries reached 49.6% and 7.2%, respectively, and the connectivity of general high angle boundaries (HABs) network was interrupted substantially by the special boundaries. However, special boundaries of fairly low fraction were developed in the specimen which was strain annealed after solution treatment and pre-ageing. The fractions of ∑3 and(∑9+∑27)boundaries was less than 35.9% and 2.5%, respectively, and the connectivity of general high angle boundaries (HABs) network was not interrupted significantly.
Key words:  Pb alloy      grain boundary character distribution (GBCD)      cold rolling and annealing      
Received:  31 August 2006     
ZTFLH:  TG111  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I5/454

[1] Palumbo G, Erb U. MRS Bull, 1999; 24(11): 27
[2] Lee D S, Ryoo H S, Hwang S K. Mater Sci Eng, 2003; A354: 106
[3] Xia S, Zhou B X, Chen W J, Wang W G. Ada Metall Sin, 2006; 42: 129 (夏爽,周邦新,陈文觉,王卫国.金属学报,2006;42:129)
[4] Wang W G, Zhou B X, Feng L, Zhang X, Xia S. Acta Metall Sin, 2006; 42: 715 (王卫国,周邦新,冯柳,张欣,夏爽.金属学报,2006; 42:715)
[5] Wang W G. Mater Sci Forum, 2007; 539-543: 3389
[6] Maitre A, Bourguignon G, Fiorani J M, Ghanbaja J, Steinmetz J. Mater Sci Eng, 2003; A358: 233
[7] Hilger J P. Power Sources, 1998; 72: 184
[8] Brandon D G. Acta Metall, 1966; 14: 1479
[9] Kaneno Y, Takasugi T. Mater Sci Eng, 2005; A393: 71
[10] Maitre A, Bourguignon G, Fiorani J M, J Steinmetz, Ghanbaja J. Mater Sci Eng, 2003; A340: 103
[11] Schuh C A, Kumar M, King W E. J Mater Sci, 2005; 40: 847
[12] Janssens K G F, Olmsted D, Holm E A, Foiles S M, Plimpton S J, Derlet P M. Nature Mater, 2006; 5: 124
[1] Bin CHEN,Jie HE,Xiaojun SUN,Jiuzhou ZHAO,Hongxiang JIANG,Lili ZHANG,Hongri HAO. Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards[J]. 金属学报, 2019, 55(6): 751-761.
[2] Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN. Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. 金属学报, 2019, 55(5): 566-574.
[3] CHEN Shu, ZHAO Jiuzhou. EFFECT OF Sn ON THE SOLIDIFICATION PROCESS AND MICROSTRUCTURE OF Al-Pb MONOTECTIC ALLOYS[J]. 金属学报, 2014, 50(5): 561-566.
[4] ZHANG Jianfeng, LE Qichi, CUI Jianzhong. EFFECT OF AC MAGNETIC FIELD ON ELECTRIC RESISTANCE OF Sn-20%Pb ALLOY[J]. 金属学报, 2013, 49(1): 101-106.
[5] ZHANG Lin WANG Engang ZUO Xiaowei HE Jicheng. EFFECT OF HIGH MAGNETIC FIELD ON THE TRANSITION BEHAVIOR OF Cu–RICH PARTICLES IN Cu–80%Pb HYPERMONOTECTIC ALLOY[J]. 金属学报, 2010, 46(4): 423-428.
[6] ZHAO Jiuzhou LI Haili WANG Qingliang ZHAO Lei HE Jie. RAPID DIRECTIONAL SOLIDIFICATION OF Al-Pb ALLOY UNDER A STATIC MAGNETIC FIELD[J]. 金属学报, 2009, 45(11): 1344-1348.
[7] Lin Zhang; Xiaowei Zuo; Jicheng He. Formation of Cu-rich Sphere Phase in Cu-80wt%Pb Hypermonotectic Alloys and the Effect of High Magnetic Field[J]. 金属学报, 2008, 44(2): 165-171 .
[8] ZHAO Jiuzhou. Liquid-liquid Phase Transformation Kinetics of an Atomized Al-Pb Alloy Drop[J]. 金属学报, 2006, 42(2): 113-117 .
[9] YAN Hongchun;HE Guanhu; ZHOU Benlian;QIN Rongshan;GUO Jingdong; SHEN Yifu(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(International Centre for Materials Physics; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1996-01-26; in revised form 1997-01-25). THE INFLUENCE OF PULSE ELECTRIC DISCHARGING ON SOLIDIFIED STRUCTURE OF Sn-10% Pb ALLOY[J]. 金属学报, 1997, 33(4): 352-358.
[10] JIA Jun;CHEN Xianchao Harbin Institute of Technology. CONTACTING FATIGUE FAILURE OF Cu-22% Pb PLAIN BEARING ALLOY[J]. 金属学报, 1989, 25(3): 76-78.
No Suggested Reading articles found!