| MICROSTRUCTURES OF NANO-TWIN STRUCTURED Cu PRODUCED BY DYNAMIC PLASTIC DEFORMATION AT LIQUID NITROGEN TEMPERATURE |
| LU Qiuhong;ZHAO Weisong; SUI Manling; LI Douxing |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室 |
|
Cite this article:
LU Qiuhong; ZHAO Weisong; SUI Manling; LI Douxing. MICROSTRUCTURES OF NANO-TWIN STRUCTURED Cu PRODUCED BY DYNAMIC PLASTIC DEFORMATION AT LIQUID NITROGEN TEMPERATURE. Acta Metall Sin, 2006, 42(9): 909-913 .
|
|
|
Abstract Microstructural feature and evolution of nano-twin bulk Cu specimens produced by means of dynamic plastic deformation at liquid nitrogen temperature (LNT-DPD) have been studied using TEM. The results show that the microstructure of LNT-DPD Cu consists of high density of nano-scaled mechanical twins, nano-sized grains and coarse grains with high density of dislocations, which makes the LNT-DPD Cu exhibit a significant high tensile yield strength. Such a deformation structure was attributed to twinning and shearing during the LNT-DPD treatment.
|
|
Received: 12 April 2006
|
|
|
[1]Varliev R Z,Islamgaliev R K,Alexandrrov I V.Prog Mater Sci,2000; 45:103 [2]Lu L,Shen Y F,Chen X H,Qian L H,Lu K.Science,2004; 304:422 [3]Meyers M A,V(?)hringer O,Lubarda V A.Acta Mater,2001; 49:4025 [4]Wang Y M,Jiao T,Ma E.Mater Trans,2003; 44:1926 [5]Christian J W,Mahajan S.Prog Mater Sci,1995; 39:1 [6]Zhao W S,Tao N R.,Guo J Y,Lu Q H,Lu K.Scr Mater,2005; 53:745 [7]Aashish R,Kenneth S,George T GⅢ.Metall Mater Trans,2001; 32A:135 [8]El-Danaf E,Kalidindi S R,Doherty R D.Metall Mater Trans,1999; 30A:1223 [9]Yamakov V,Wolf D,Phillpot S R,Gleiter H.Acta Mater,2002; 50:5005 [10]Blewitt T H,Coltman R R,Redman J K.J Appl Phys,1957; 28:651 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|