| Thermal Stability of A Novel Ti-Si-C-N Superhard Nanocomposite Coating at Elevated Temperature |
| Yan Guo |
| 西安交通大学材料学院国家重点实验室 |
|
Cite this article:
Yan Guo. Thermal Stability of A Novel Ti-Si-C-N Superhard Nanocomposite Coating at Elevated Temperature. Acta Metall Sin, 2006, 42(2): 172-176 .
|
|
|
Abstract Superhard nanocomposite Ti-Si-C-N coatings were deposited on substrate of high speed steel using an industrial pulsed d.c. plasma chemical vapor deposition set-up. Dependence of Si and C contents and annealing at elevated temperatures on the microstructure and hardness of Ti-Si-C-N coatings were investigated. Detailed microstructure examined by means of X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and transmission electron microscopy (TEM) suggested that the Ti-Si-C-N coatings was a nanocomposite structure composed of nanocrystalline Ti(C,N) and amorphous carbon and Si3N4. And the crystalline size and microhardness of coatings showed high thermal stability even at 1000° C when Si and C contents were higher of 12.1 at.% Si, 32.9 at.% C. The possible origin of high thermal stability of superhard nanocomposite Ti-Si-C-N coatings is explained by spinodal decomposition that occurs during deposition.
|
|
Received: 20 May 2005
|
|
|
[1] Ma S L, Xu K W, Jie W Q. J Vac Sci Technol, 2004; B22: 1694 [2] Veprek S, Reiprik S, Li S Z. Appl Phys Lett, 1995; 66: 2640 [3] Ma Q S, Ma S L, Xu K W. J Vac Sci Technol, 2005; A23(1): 12 [4] Ma S L, Xu K W. Acta Metall Sin, 2004; 40: 669(马胜利,徐可为.金属学报,2004;40:669) [5] Ma S L, Xu K W. Chin J Nonfer Met, 2000; 10: 489(马胜利,徐可为.中国有色金属学报,2000;10:489) [6] Jeon J H, Choi S R, Chung W S, Kim K H. Surf Coat Technol, 2004; 188-189: 415 [7] Kuo D H, Liao W C. Appl Surf Sci, 2002; 199: 278 [8] Ma D Y. PhD Thesis, Xi'an Jiaotong University, 2005(马大衍.西安交通大学博士学位论文,2005) [9] Veprek S, Niederhofer A, Moto K, Botom T, Mannling H D, Nesladek P, Dollinger G. Surf Coat Technol, 2000; 133-134: 152 [10] Ma S L, Prochazka J, Karvankova P, Ma Q S, Niu X P, Ma D Y, Xu K W. Surf Coat Technol, 2005; 194: 143 [11] Kuo D H, Huang K W. Thin Solid Films, 2001; 394: 81 [12] Kuo D H, Liao W C. Thin Solid Films, 2002; 419: 11 [13] Guo Y, Chang G R, Ma S L, Xu K W. Acta Metall Sin, 2005; 41: 985(郭岩,畅庚榕,马胜利,徐可为.金属学报,2005;41:985) [14] Kim K H, Choi S R, Yoon S Y. Surf Coat Technol, 2002; 298: 243 [15] Veprek S, Haussmann M, Reiprich S, Dian J, Li S Z. Surf Coat Technol, 1996; 86/87: 394 [16] Ma D Y, Ma S L, Xu K W. Chin J Mater Res, 2004; 18: 617(马大衍,马胜利,徐可为.材料研究学报,2004;18:617) [17] Mannling H D, Patil D S, Moto K, Jilek M, Veprek S. Surf Coat Technol, 2001; 146-147: 263 [18] Veprek S, Veprek H, Maritza G J, Karvankova P. Thin Solid Films, 2005; 476: 1Z |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|