Please wait a minute...
Acta Metall Sin  2005, Vol. 41 Issue (6): 633-637     DOI:
Research Articles Current Issue | Archive | Adv Search |
Oxidation Behaviors of Ti44Ni47Nb9 Shape Memory Alloy at High Temperature
TAO Binwu; LIU Jianhua; LI Songmei
School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083
Cite this article: 

TAO Binwu; LIU Jianhua; LI Songmei. Oxidation Behaviors of Ti44Ni47Nb9 Shape Memory Alloy at High Temperature. Acta Metall Sin, 2005, 41(6): 633-637 .

Download:  PDF(349KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The isothermal oxidation resistance of Ti44Ni47Nb9 shape memory alloy (SMA) in air over the temperature range of 450-850 ℃ was studied by using XRD, SEM and EDS techniques. Light oxidation was found on the alloy surface at 450 ℃. The alloy was attacked by oxidation and the oxidation kinetic curves were approximately parabola within the temperature range of 600—800 ℃. Experimental results indicate that a multi-layered scale was formed, consisting of an outer rutile layer, a Nb rich intermediate layer and a thin inner Ni3Ti layer. It was found that the Nb rich intermediate layer was compact, which obviously improved the oxidation resistance of the alloy due to its effective inhibition to diffusion of oxygen and titanium. Furthermore, the internal oxidation of nickel element was also inhibited because of the existence of Nb rich layer, which reduced oxygen concentration in the alloy.
Key words:  Ti44Ni47Nb9      shape memory alloy      high temperature      
Received:  14 September 2004     
ZTFLH:  TG174  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2005/V41/I6/633

[1]Kajiwara S.Mater Sci Eng,1999;A273-275:67
[2]Piao M,Miyazakai S,Otsuka K.Mater Trans JIM,1992; 33:337
[3]Cai W,Zhang C C.J Mater Sci Technol,1994;10:27
[4]Yang H B,Yin W H,Lin J Y,Zhang X M,Guo J H.Rare Met Mater Eng,1999;28:81 (杨华斌,殷为宏,吝靖玉,张小明,郭继红.稀有金属材料与工程,1999;28:81)
[5]Dong Z Z,Liu W X,Jia D,Tang Z L,Wang D F.Rare Met Mater Eng,2000;29:182 (董治中,刘文西,贾堤,唐子龙,王德法.稀有金属材料与工程,2000;29:182)
[6]Mo H Q,Li C,Wang C L,Qiu S Y,Huang D C,Shen B L.Nucl Power Eng,2003;24:559 (莫华强,李聪,王丛林,邱绍宇,黄德成,沈保罗.核动力工程,2003;24:559)
[7]Long N D,Zhu J H.Rare Met Mater Eng,2003;32:740 (龙霓东,朱金华.稀有金属材料与工程,2003;32:740)
[8]He X M,Rong L J,Yan D S,Jiang Z M,Li Y Y.Ada Metall Sin,2004;40:721 (何向明,戎利建,阎德胜,姜志民,李依依.金属学报,2004;40:721)
[9]Xu C H,Ma X Q,Shi S Q,Wo C H.Mater Sci Eng,2004;A371:45
[10]Liu Y H.Theory of Metal Corrosion.Beijing:Aeronautics Industry Press,1993:186 (刘永辉.金属腐蚀原理.北京:航空工业出版社,1993:186)
[11]Gesmundo F,Niu Y,Viani F.Oxid Met,1996;46:441
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi. Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 55-74.
[4] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[5] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[6] ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong. Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy[J]. 金属学报, 2022, 58(8): 1065-1071.
[7] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[8] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[9] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite[J]. 金属学报, 2021, 57(7): 921-927.
[10] YE Junjie, HE Zhirong, ZHANG Kungang, DU Yuqing. Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy[J]. 金属学报, 2021, 57(6): 717-724.
[11] XU Jinghui, LI Longfei, LIU Xingang, LI Hui, FENG Qiang. Thermal-Stress Coupling Effect on Microstructure Evolution of a Fourth-Generation Nickel-Based Single-Crystal Superalloy at 1100oC[J]. 金属学报, 2021, 57(2): 205-214.
[12] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[13] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[14] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[15] CHEN Xiang,CHEN Wei,ZHAO Yang,LU Sheng,JIN Xiaoqing,PENG Xianghe. Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. 金属学报, 2020, 56(3): 361-373.
No Suggested Reading articles found!