| SIMULATIONS AND ANALYSIS OF PHASE TRANSFORMATIONS IN bcc-Fe UNDER ISOTHERMAL COMPRESSION |
| ;; |
| 北京应用物理与计算数学研究所 |
|
Cite this article:
. SIMULATIONS AND ANALYSIS OF PHASE TRANSFORMATIONS IN bcc-Fe UNDER ISOTHERMAL COMPRESSION. Acta Metall Sin, 2008, 44(9): 1085-1089 .
|
|
|
Abstract Using EAM potential and molecular dynamics (MD), we simulate the transition (bcc to hcp) in bcc-Fe under isothermal compression (along [001] orientation). Simulated results reveal that while stress beyond transition threshold, hcp nucleations appear and form flaky grains along (110) face and the system shows an over-relaxation of stress. Mean stress and hcp mass percent increase linearly with volume compression during the growth of hcp nucleations, and longitudinal deviatonic stress reduces linearly with hcp mass percent for the whole transition process. Average potential of hcp atoms are greater than those of bcc atoms.
|
|
Received: 21 December 2007
|
|
|
[1]Bancroft D,Peterson E L,Minshall S.J App Phys,1956; 27:291 [2]Johnson P C,Stein B A,Davis R S.J Appl Phys,1962; 33:557 [3]Takahashi T,Bassett W A.Science,1964;145:483 [4]Barker L M,Hollenbach R E.J Appl Phys,1974;45:4872 [5]Taylor R D,Pasternak M P,Jeanloz R.J Appl Phys,1991; 69:6126 [6]Boettger J C,Wallace D C.Phys Rev,1997;55B:2840 [7]Yano K,Horie Y.Int J Plast,2002;18:1427 [8]Caspersen K J,Lew A,Ortiz M,Carter E A.Phys Rev Left,2004;93:115501 [9]Daw M S,Baskes M I.Phys Rev,1984;29B:6443 [10]Finnis M W,Sinclair J E.Philos Mag,1984;50A:45 [11]Kadau K,Germann T C,Lomdahl P S,Holian B L.Sci- ence,2002;296:1681 [12]Kadau K,Germann T C,Lomdahl P S,Holian B L.Phys Rev,2005;72B:064120 [13]Shao J L,Wang P,Qin C S,Zhou H Q.Acta Phys Sin, 2007;56:5389 (邵建立,王裴,秦承森,周洪强.物理学报,2007;56:5389) [14]Shao J L,Wang P,Qin C S,Zhou H Q.Acta Phys Sin, 2008;57:1254 (邵建立,王裴,秦承森,周洪强.物理学报,2008;57:1254) [15]Harrison R J,Voter A F,Chen S P.Atomistic Simulation of Materials Beyond Pair Potentials.New York:Plenum Press,1989:219 [16]Rose J H,Smith J R,Guinea F,Ferrante J.Phys Rev, 1984;29B:2963 [17]Hoffmann K H,Schreiber M.Computational Physics. Berlin:Springer-Verlag,1996:268 [18]Swope W C,Andersen H C,Berens P H,Wilson K R.J Chem Phys,1982;76:637 [19]Irving J H,Kirkwood J G.J Chem Phys,1950;18:817 [20]Allen M P,Tildesley D J.Computer Simulation of Liquids. Oxford:Clarendon Press,1987:46 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|