| Nucleation Model in Solidification Processes of the Alloys |
| CHEN Zhongwei; JIE Wanqi |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
CHEN Zhongwei; JIE Wanqi. Nucleation Model in Solidification Processes of the Alloys. Acta Metall Sin, 2004, 40(10): 1027-1031 .
|
|
|
Abstract An experiential nucleation model in solidification processes of the
industrial alloys was established by introducing the experimental
parameters. This model not only described nucleation rate of the
alloys quantitatively, but also linked the nucleation rates with the
final grain sizes. The surface area of effective catalysts per unit
volume melt and the contact angle of effective catalysts
in the melt in solidification processes were calculated
with the model and the nucleation characteristic of the casting was
analyzed. The model was also used to estimate the nucleation parameters
of Al-7Si alloy and Al-7Si-0.55Mg alloy in the definite melting
condition.
|
|
Received: 14 May 2004
|
|
|
[1] Turnbull D. J Appl Phys, 1950; 21: 1022 [2] Turnbull D. J Chem Phys, 1950; 18: 198 [3] Maxwell I, Hellawell A. Acta Metall, 1975; 23(2) : 229 [4] Wei B B, Yang G C, Zhou Y H. Ada Mater, 1991; 39:1249 [5] Turbull D, Cech R E. J Appl Phys, 1950; 21: 804 [6] Jian Z Y, Chang F E, Ma W H. Sci Chin, 2000; 43E(2) :113 [7] Thompson C V, Spaepen F. Ada Metall, 1983; 31: 2021 [8] Zhang X Z. Ada Mater, 1998; 46: 1135 [9] Uolland-Moritz D, Schroess J, Herlach D M. Ada Mater,1998; 46: 1601 [10] Rappaz M, Gandin C A. Ada Metall Mater, 1993; 41(2) : 345 [11] Thevoz Ph, Desbiolles J L, Rappaz M. Metall Mater TransA, 1989; 20A: 311 [12] Christian J W. The Theory of Transformation in Metalsand Alloys. Pergamon, Oxford, 1975: 418 [13] Turnbull D. In: Seitz F, Turbull D eds, Solid StatePhysics. New York: Academic Press, 1956: 225 [14] Spaepen F, Turnbull D. In: Grant N J, Giessen B C eds,Proc 2nd Int Conf On Rapidly Quenched Metals. Cambridge: MIT Press, 1976: 205 [15] Spaaepen F. Acta Metall, 1975; 23: 729 [16] Spaepen F, Meyer R B. Scr Metall, 1976; 10(1) : 37 [17] Turnbull D. Contemporary Phys, 1969; 10: 473 [18] Mueller B A, Perepezko J H. Metall Mater Trans A, 1987;18A: 1143 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|