| Size and Shape Dependent Melting--Thermodynamic Properties of Metallic Nanoparticles |
| XIE Dan; QI Weihong; WANG Mingpu |
| Department of Materials Science and Engineering; Central SouthUniversity; Changsha 410083 |
|
Cite this article:
XIE Dan; QI Weihong; WANG Mingpu. Size and Shape Dependent Melting--Thermodynamic Properties of Metallic Nanoparticles. Acta Metall Sin, 2004, 40(10): 1041-.
|
|
|
Abstract A melting--thermodynamic model is developed, which can describe the
effect of size and shape of metallic nanoparticle on its
melting--thermodynamic properties. It is predicted that there exist
a minimum critical size
and a lowest melting temperature
for
metallic nanoparticle. The present theoretical results on the melting
point, the melting entrapy and the melting enthalpy of nanoparticles
Au, In, Al and Sn are consistent with the corresponding experimental
values.
|
|
Received: 13 November 2003
|
|
|
[1] Hill T L. In: Benjamin W A ed. Themodynamics of SmallSystems. NewYork: INC, 1963: 6 [2] Wautelet M, Dauchot J P, Hecq M. J Phys Condens Matter, 2003; 15: 3651 [3] Wautelet M, Dauchot J P, Hecq M. Mater Sci Eng, 2003;23: 187 [4] Qi W H, Wang M P, Xu G Y. J Mater Sci Lett, 2003; 22:1333 [5] Qi W H, Wang M P, Xu G Y. Chem Phys Lett, 2003; 372:632 [6] Xie D, Qi W H, Wang M P. Physica B, in submitted [7] Li C H, Joo Lim Hoe, Wu P. J Phys Chem of Solids, 2003;64: 201 [8] Mott N F. Proc Roy Soc, 1934; 146A: 465 [9] Regel' A R, Glazov V M. Semiconductors, 1995; 29(5) :405 [10] Jiang Q, Nan S H, Zhou M. Acta Metall Sin, 1998; 34:870(蒋青,南胜辉,周明.金属学报,1998;34:870) [11] Jiang Q, Zhang Z, Wang Y W. Mater Sci Eng, 2000; 286A:139 [12] Jiang Q, Shi H X, Zhao M. J Chem Phys, 1999; 111: 2176 [13] Xie D, Qi W H, Wang M P. J Mater Sci Lett, in submitted [14] Zhao M, Zhou X H, Jiang Q. J Mater Res, 2001; 16: 3304 [15] Jiang Q, Yang C C, Li J C. Mater Lett, 2002; 56: 1019 [16] Ph Buffat, J P Borel. Phys Rev A, 1976; 13: 2287 [17] Frank G Shi. J Mater Res, 1994; 9: 1307 [18] Zhang Z, Lu X X, Jiang Q.Physica B, 1999; 270: 249 |