| EFFECTS OF SPUTTERING PARAMETER ON THE MICROSTRUCTURE OF Ti--6Al--4V COATING ON SiC FIBRE |
| WANG Yumin; FU Yuechun; SHI Nanlin; ZHANG Dezhi; YANG Rui |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
WANG Yumin; FU Yuechun; SHI Nanlin; ZHANG Dezhi; YANG Rui. EFFECTS OF SPUTTERING PARAMETER ON THE MICROSTRUCTURE OF Ti--6Al--4V COATING ON SiC FIBRE. Acta Metall Sin, 2004, 40(4): 359-362 .
|
|
|
Abstract The effects of sputtering parameters on the microstructure of Ti--6Al--4V coating on SiC(f) prepared by magnetron sputtering were studied. The results show that the deposition rate is related to the working pressure at a given power density. The morphology
of the deposited layer and its binding with the fibre are dependent on temperature. The composition of the coat is close to Ti--6Al--4V, and is uniform throughout the thickness of the coat. The deposited layer
consists of crystallites with nonequilibrium hcp structure with grain size of 20---50 nm. The interface between SiC fibre and Ti--6Al--4V coating was investigated by scanning electron microcopy and energy dispersive X--ray spectroscopy. The examination
reveals no chemical reaction at the fibre--coat interface which is in nature a sharp interface formed by bonding of the two substances.
|
|
Received: 24 February 2003
|
|
|
[1] Doychak J. JOM, 1992; 44(6) : 46 [2] GUO Z X, Derby B. Prog Mater Sci, 1995; 39: 411 [3] Das G. Metall Trans, 1990; 21A: 1571 [4] Subramanian P R, Krishnamurthy S, Keller S T, Mendi-ratta M G. Mater Sci Eng, 1988; 244A: 1 [5] Tang W Z. Principles, Technology and Application of ThinFilm Materials. 1st ed., Beijing: Metallurgy IndustryPress, 1998(唐伟忠.薄膜材料制备原理、技术及应用,第1版.北京:冶金工业出版社,1998) [6] Kunze J M, Wadley H N G. Mater Sci Eng, 1998; 244A: 138 |