Acta Metall Sin  2004, Vol. 40 Issue (4): 363-366     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECT OF CONSTRAINT TRANSFORMATION ON RECOVERY STRAIN OF Ti44Ni47Nb9 ALLOY
LIU Xiaopeng; JIN Wei; CAO Mingzhou; YANG Rui
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

LIU Xiaopeng; JIN Wei; CAO Mingzhou; YANG Rui. EFFECT OF CONSTRAINT TRANSFORMATION ON RECOVERY STRAIN OF Ti44Ni47Nb9 ALLOY. Acta Metall Sin, 2004, 40(4): 363-366 .

Download:  PDF(183KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of constraint transformation heating temperature Th on the free reverse transformation behavior of 10\% strained Ti44Ni47Nb9 alloy was investigated, and the experimental results showed that after the first constraint transformation the strained Ti44Ni47Nb9 alloy exhibits two separate recovery strains εr1 and εr2 on subsequent free reverse transformation, which increases and decreases with increasing Th, respectively. However, the total recovery strain εr(εr=εr1+εr2)of Ti44Ni47Nb9 alloy decreases with increasing Th. The plastic strain of Ti44Ni47Nb9 alloy is increased by the deformation of martensite under the recovery stress during the constraint transformation, which decreases εr strain of Ti44Ni47Nb9 alloy. Since the martensite of strained Ti44Ni47Nb9 alloy is consisted of M1 and M2 oriented martensites with different strain levels after the first constraint transformation, strains εr1 and εr2 are related to M1 and M2 oriented martensite reverse transformations respectively.
Key words:  Ti44Ni47Nb9 alloy      constraint transformation      recovery strain      
Received:  16 April 2003     
ZTFLH:  TG146.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I4/363

[1] Metlon K N, Simpson J, Duerig T W. Proc Int Conf on Martensitic Trans, 1986: 1053
[2] Melton K N, Proft J L, Duerig T W. Prog MRS Int Meeting on Advance Mater, 1988; 9: 165
[3] Zhao L C, Duerig T W, Justi S, Melton K N, Proft J L, Yu W, Wayman C M. Scr Metall Mater, 1990; 24: 221
[4] Cai W, Zhang C S, Zhao L C. J Mater Sci Technol, 1994; 10: 27
[5] Madagopal K, Ganesh R Krishnan, Banerjee S. Scr Metall, 1988; 22: 1593
[6] Brinson L C. J Intell Mater Syst Struct, 1993; 4: 229
[7] Wen Y H, Li N, Tu M J. Scr Mater, 2001; 44: 1113
[8] Piao M, Otsuka K, Miyazaki S, Horikawa H. Mater Trans JIM, 1993; 34: 919
[9] Lin H C, Wu S K. Ada Metall Mater, 1994; 42: 1623
[10] Liu X P, Jin W, Cao M Z, Yang D Z, Chen F X. Acta Metall Sin, 2002; 38: 193(刘晓鹏,金伟,曹名洲,杨大智,陈(?)(?).金属学报,2002;38:193)
[1] LIU Xiaopeng; JIN Wei; CAO Mingzhou; YANG Rui. Study on Constraint Transformation Behavior of Tini Alloy[J]. 金属学报, 2004, 40(2): 130-134 .
No Suggested Reading articles found!