| DISSOLUTION OF THE SECOND PHASE DURING CONTINUOUS HEATING PROCESS |
| WANG Xiaoying; ZHANG Ruijie; JIE Wanqi |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
WANG Xiaoying; ZHANG Ruijie; JIE Wanqi. DISSOLUTION OF THE SECOND PHASE DURING CONTINUOUS HEATING PROCESS. Acta Metall Sin, 2004, 40(4): 434-438 .
|
|
|
Abstract A dissolution model of the plate--like and spherical second phases in the multiphase alloy during continuous heating process with constant rate has been proposed. The effects of heating rate and interface curvature on the
concentration profiles in the matrix and the dissolution rate of the second phase were discussed. The model was applied to calculate the dissolved fraction of the second phase before melting during heating process. The
calculated results for Al--5.8%Cu alloys, where the eutectic melting fraction of the non--equilibrium eutectic was determined by DSC analysis, agree well with the experimental ones, clearly indicating the validity of the developed model.
|
|
Received: 16 April 2003
|
|
|
[1] Rovira M M, Lancini B C, Robert M H. J Mater ProcTechnol, 1999; 92-94: 42 [2] Aaron H B, Kotler G R. Metall Trans, 1971; 2: 393 [3] Aaron H B, Fsinstein D, Kotler G R. J Appl Phys, 1970;41(11) : 4404 [4] Baty D L, Tanzilli R A, Heckel R W. Metall Trans, 1970; 1: 1651 [5] Nolfi F V, Shewmon P G, Foster J S. Metall Trans, 1970;1: 789 [6] Frade J R. J Mater Sci, 1997; 32: 3549 [7] Liang K M. Methods of Mathematical Physics, Beijing:High Education Press, 1998: 216(梁昆淼.数学物理方法.第3版,北京:高等教育出版社,1998:216) [8] Xie F Y, Kraft T, Zuo Y, Moon C H, Chang Y A. Ada Mater, 1999; 47(2) : 489 [9] Eric A B. Simithells Metals Reference Book, UK: Butter-worths & Co.Ltd., 1976: 11 [10] Hatch J E. Aluminum: Properties and Physical Metallurgy, USA: A.S. M, 1983: 47 |
| No Suggested Reading articles found! |
|
|