| Dislocation Pattern in Deformation Band and Crack Nucleation in a Fatigued Copper Bicrystal with Perpendicular Grain Boundary |
| LI Yong; LI Shouxin; LI Guangyi |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
LI Yong; LI Shouxin; LI Guangyi. Dislocation Pattern in Deformation Band and Crack Nucleation in a Fatigued Copper Bicrystal with Perpendicular Grain Boundary. Acta Metall Sin, 2004, 40(5): 462-466 .
|
|
|
Abstract The dislocation pattern evolution and crack nucleation in a fatigued
copper bicrystal with perpendicular grain boundary (GB) have been
investigated by electron channelling contrast
(ECC) technique in SEM. The observation results
show that in the process from the formation of
deformation band (DB) to the appearance of fatigued
crack, the spacing between the wall
structures in DB keeps constant. The
dislocation pattern around the crack tips of transgranular and
granular presents misorientation cell structure. The crack
preferentially form in DB.
|
|
Received: 18 April 2003
|
|
|
[1] Essmann U, Gosele U, Mughrabi H. Philos Mag, 1981; 44A: 405 [2] Basinski Z S, Basinski J S. Acta Metall, 1985; 33:1319 [3] Ma B T, Laird C. Acta Metall, 1989; 37:325 [4] King A E, Teer D G. Philos Mag, 1967; 15:425 [5] Chin G Y, Backofen W A. J Inst Met, 1961-62; 90:13 [6] Saletore M, Taggart R. Mater Sci Eng, 1978; 36:259 [7] Li S X, Li Y, Li G Y, Wang Z G, Lu K. Philos Mag, 2002; 82A: 867 [8] Li S X, Li X W, Zhang Z F, Wang Z G. Philos Mag, 2002; 82A: 3129 [9] Li Y, Li S X, Li G Y, Lu K. Z Metallkd, in press [10] Bayerlein M, Mughrabi H. Acta Metall Mater, 1991; 39: 1645 [11] Polak J, Obrtllik K, Lisskutin P. In: Lukas P, Polak J, eds., Basic Mechanisms in Fatigue of Metals, Amsterdam: Academia and Elsevier, 1988:101 [12] Kim W H, Laird C. Acta Metall, 1978; 26:777 [13] Kim W H, Laird C. Acta Metall, 1978: 26:789 [14] Lim L C, Tay Y K, Fong H S. Acta Metall Mater, 1990; 38:595 [15] Ahmed J, Wilkinson A J, Roberts S G. Philos Mag, 2001; 81A: 1473 [16] Hunsche A, Neumann P. Acta Metall, 1986; 34:207 [17] Katagiri K. Omura A, Koyanagi K, Awatani J, Shiraishi T. Kaneshiro H, Metall Trans, 1977; 8A: 1769 [18] Brown L M. Met Sci, 1977; 11:315 [19] Lin M R, Fine M E, Mura T. Acta Metall, 1986; 34: 619 [20] Zhai T, Martin J W, Briggs G A D, Wilkinson A J. Acta Mater, 1996; 44:3477 [21] Li X W, Wang Z G, Li S X. Philos Mag, 2000; 80A: 1901 |