| A New Aging Precipitated Phase in NiTi Alloy |
| XU Aiqun |
| Analysis and Testing Center; Southeast University; Nanjing 210096 |
|
Cite this article:
XU Aiqun. A New Aging Precipitated Phase in NiTi Alloy. Acta Metall Sin, 2004, 40(2): 125-129 .
|
|
|
Abstract The phase constitution of a highly dense NiTi alloy prepared by
combustion synthesis and treated at high temperature solution and
aging was analyzed by X--ray diffraction and transmission electron
microscopy (TEM). Two kinds of fine precipitates exist in the alloy
besides Ti2Ni. One is the rhombohedral structure Ti11Ni14
(Ti3Ni4}) with a=0.67 nm and alpha=113.85 circ,
which has an orientation relationship with the matrix
(B2 structure, a=0.302 nm):
<111$>Ti11Ni14∥<111>B2,
{1-10>Ti11Ni14∥{123}B2. Another
one is an unreported metastable precipitate with a long range ordered
structure caused by Ni at the positions of Ti in NiTi phase. Its lattice
parameter (a=0.873 nm) is about 3 times of that of NiTi matrix and the
molecular formula is Ti13Ni14.
|
|
Received: 16 April 2003
|
|
|
[1] Yi H C, Moore J J. J Mater Sci, 1992; 27: 5067 [2] Funakubo K ed., translate by Qian D F. Shape Memory Alloy. Beijing: China Machine Press, 1984: 85(舟久保 熙康编,千冬范译.形状记忆合金.北京:机械工业出版社,1984:85) [3] He Z R. Funct Mater, 1998; 29: 157(贺志荣.功能材料,1998;29:157) [4] He Z R, Zhang Y H, Miyazaki S. Met Heat Treat, 1996; (10) : 7(贺志荣,张永宏,宫崎修一.金属热处理,1996;(10) :7) [5] Nishida M, Wayman C M, Honma T. Metall Trans, 1986; 17A: 1505 [6] Hwang C M, Meichle M, Salamon M B, Wayman C M. Philos Mag, 1983; 47A: 31 [7] The Metallography and Heat Treatment Teaching and Research Group of Beijing Steel College. Metal Heat Treatment. Beijing: China Industry Press, 1961: 135(北京钢铁学院金相及热处理教研组.金属热处理.北京:中国工业出版社,1961:135) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|