| Study on Constraint Transformation Behavior of Tini Alloy |
| LIU Xiaopeng; JIN Wei; CAO Mingzhou; YANG Rui |
| Institute of Metal Research; The Chinese Academy of Sciences; |
|
Cite this article:
LIU Xiaopeng; JIN Wei; CAO Mingzhou; YANG Rui. Study on Constraint Transformation Behavior of Tini Alloy. Acta Metall Sin, 2004, 40(2): 130-134 .
|
|
|
Abstract The constraint transformation behavior of 7% strained TiNi alloy was
investigated, and the experimental results show that the recovery stress
formed at the first constraint transformation thermal cycling is the
highest, and then decreases with increasing the constraint transformation
thermal cycling number. It is indicated that the recovery strain of
deformed TiNi alloy is decreased with increasing the constraint transformation
thermal cycling number by forming the internal plastic deformation,
which results in the decrease of the recovery stress. The reverse
transformation start temperature As' of the deformed TiNi
alloy at the first constraint transformation thermal cycling is elevated
to a higher temperature, but it nearly returns to the original value of
undeformed one at subsequent constraint transformation thermal cycling,
and does not change with increasing the constraint transformation thermal
cycling number.
|
|
Received: 24 February 2003
|
|
|
[1] Sittner P, Vokoun D, Dayananda G N, Stalmans R. Mater Sci Eng, 2000; A286: 298 [2] Cai W. Zhang C S, Zhao L C. J Mater Sci Technol, 1994: 10: 27 [3] Liu Y. Xie Z. van Humbeeck J. Delaey L. Acta Mater, 1998: 46: 4325 [4] Liu Y N. Liu Y, van Humbeeck J. Acta Mater, 1999; 47: 199 [5] Piao M, Otsuka K. Miyazaki S, Horikawa H. Mater Trans JIM. 1993; 34: 919 [6] Liu X P. Jin W, Cao M Z, Yang D Z, Chen F X. Acta Metall Sin. 2002; 38: 193(刘晓鹏,金伟,曹名洲,杨大智,陈騑騢.金属学报,2002;38:193) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|