| Evolution of Microstrucutre During Static Recrystallization in FGH96 Superalloy |
PENG Zichao1( ), LUO Junpeng2, ZHAO Yu3, ZHOU Lei1, WANG Xuqing1, ZOU Jinwen1 |
1 Science and Technology on Advanced High Temperature Structural Materials Laboratory, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China 2 AECC South Industry Co. Ltd., Zhuzhou 412002, China 3 AECC Hunan Aviation Powerplant Research Institute, Zhuzhou 412002, China |
|
Cite this article:
PENG Zichao, LUO Junpeng, ZHAO Yu, ZHOU Lei, WANG Xuqing, ZOU Jinwen. Evolution of Microstrucutre During Static Recrystallization in FGH96 Superalloy. Acta Metall Sin, 2025, 61(2): 235-242.
|
|
|
Abstract FGH96 alloy is a nickel-based superalloy that is commonly used in fabricating the turbine disks of aero engines owing of its excellent mechanical properties. Because the properties of nickel-based superalloys are determined based on their microstructure, researchers have been studying the evolution of microstructure in FGH96. However, most studies have focused on FGH96 superalloys that have undergone a hot isostatic pressing (HIP) process or a combination of HIP and hot isostatic forging. Recently, hot extrusion (HEX) has been widely used for manufacturing FGH96 superalloys; however, the research on alloys manufactured via HEX is scarce. In this study, FGH96 superalloys were solution heat-treated at temperatures ranging from 1100 oC to 1260 oC, and the evolution of their microstructure was analyzed via OM, EBSD, and TEM techniques. The mechanism of static recrystallization and the formation mechanism of Σ3 twin boundaries were also investigated. The results showed that the static recrystallization grain size and grain boundaries, including small angle boundaries, large angle boundaries, and Σ3 twin boundaries, were substantially influenced by the solution temperature. Furthermore, a distinct correlation existed between the microstructure evolution and solution temperature. The static recrystallization in the FGH96 alloy mainly occurs through the nucleation and growth of subgrains at temperatures ranging from 1100 oC to 1260 oC. During the static recrystallization process, a large number of stacking faults formed at the () close-packed plane, which improved the free energy. Therefore, to reduce the free energy, subsequent atoms were stacked symmetrically to the stacking faults, leading to the formation of Σ3 twin boundaries.
|
|
Received: 24 October 2022
|
|
|
Corresponding Authors:
PENG Zichao, professor, Tel: (010)62498272, E-mail: pengzichaonba@126.com
|
| 1 |
Zou J W, Wang W X. Development and application of P/M superalloy [J]. J. Aeronaut. Mater., 2006, 26(3): 244
|
|
邹金文, 汪武祥. 粉末高温合金研究进展与应用 [J]. 航空材料学报, 2006, 26(3): 244
|
| 2 |
Zhang G Q, Zhang Y W, Zheng L, et al. Research progress in powder metallurgy superalloys and manufacturing technologies for aero-engine application [J]. Acta Metall. Sin., 2019, 55: 1133
doi: 10.11900/0412.1961.2019.00119
|
|
张国庆, 张义文, 郑 亮 等. 航空发动机用粉末高温合金及制备技术研究进展 [J]. 金属学报, 2019, 55: 1133
doi: 10.11900/0412.1961.2019.00119
|
| 3 |
Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1
|
| 4 |
Wang X Q, Luo X J, Zou J W. Effects of HIP temperature on microstructure of FGH96 superalloy [J]. J. Aeronaut. Mater., 2006, 26(3): 293
|
|
王旭青, 罗学军, 邹金文. 热等静压温度对FGH96粉末高温合金显微组织的影响 [J]. 航空材料学报, 2006, 26(3): 293
|
| 5 |
Zou J W, Liu D, Liu B C, et al. Simulation of wind chill process for turbine disk [J]. J. Mater. Eng., 2009, (10): 7
|
|
邹金文, 刘 东, 柳百成 等. 涡轮盘风冷过程数值模拟研究 [J]. 材料工程, 2009, (10): 7
|
| 6 |
Li J R, Xiong J C, Tang D Z. Advanced High Temperature Structural Materials and Technology [M]. Beijing: National Defense Industry Press, 2012: 181
|
|
李嘉荣, 熊继春, 唐定中. 先进高温结构材料与技术 [M]. 北京: 国防工业出版社, 2012: 181
|
| 7 |
Hu B F, Chen H M, Jin K S, et al. Static recrystallization mechanism of FGH95 superalloy [J]. Chin. J. Nonferrous Met., 2004, 14: 901
|
|
胡本芙, 陈焕铭, 金开生 等. FGH95高温合金的静态再结晶机制 [J]. 中国有色金属学报, 2004, 14: 901
|
| 8 |
Huang G C, Liu G Q, Feng M N, et al. Effect of solution heat treatment on microstructure and properties of FGH95 alloy [J]. Trans. Mater. Heat Treat., 2017, 38: 71
|
|
黄国超, 刘国权, 冯敏楠 等. 固溶热处理工艺对FGH95合金组织和性能的影响 [J]. 材料热处理学报, 2017, 38: 71
|
| 9 |
Liu J T, Liu G Q, Hu B F, et al. Study on the static recrystallization of FGH96 superalloy [J]. Trans. Mater. Heat Treat., 2005, 26: 12
|
|
刘建涛, 刘国权, 胡本芙 等. FGH96合金静态再结晶行为的研究 [J]. 材料热处理学报, 2005, 26: 12
|
| 10 |
Ning Y Q, Yao Z K. Recrystallization nucleation mechanism of FGH4096 powder metallurgy superalloy [J]. Acta Metall. Sin., 2012, 48: 1005
|
|
宁永权, 姚泽坤. FGH4096粉末高温合金的再结晶形核机制 [J]. 金属学报, 2012, 48: 1005
doi: 10.3724/SP.J.1037.2012.00116
|
| 11 |
Ning Y Q, Fu M W, Yao W. Recrystallization of the hot isostatic pressed nickel-base superalloy FGH4096. II: Characterization and application [J]. Mater. Sci. Eng., 2012, A539: 101
|
| 12 |
Watanabe T. An approach to grain boundary design for strong and ductile polycrystals [J]. Res. Mech., 1984, 11: 47
|
| 13 |
Jin Y, Lin B, Bernacki M, et al. Annealing twin development during recrystallization and grain growth in pure nickel [J]. Mater. Sci. Eng., 2014, A597: 295
|
| 14 |
Bair J L, Hatch S L, Field D P. Formation of annealing twin boundaries in nickel [J]. Scr. Mater., 2014, 81: 52
|
| 15 |
Randle V. The coincidence site lattice and the ‘sigma enigma’ [J]. Mater. Charact., 2001, 47: 411
|
| 16 |
Lu L, Shen Y F, Chen X H, et al. Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422
pmid: 15031435
|
| 17 |
Yuan Y, Gu Y F, Cui C Y, et al. A novel strategy for the design of advanced engineering alloys—Strengthening turbine disk superalloys via twinning structures [J]. Adv. Eng. Mater., 2011, 13: 296
|
| 18 |
Peng Z C, Zou J W, Wang Y, et al. Effects of solution temperatures on creep resistance in a powder metallurgy nickel-based superalloy [J]. Mater. Today Commun., 2021, 28: 102573
|
| 19 |
Li Z G. Evolution of annealing twin boundary and mechanical behavior in a nickel-iron based wrought alloy [D]. Shanghai: Shanghai Jiao Tong University, 2015
|
|
李志刚. 一种镍铁基变形高温合金中退火孪晶界的演变与力学行为 [D]. 上海: 上海交通大学, 2015
|
| 20 |
Fang B, Ji Z, Tian G F, et al. Investigation on complete solution temperature of γ′ in the P/M superalloy of FGH96 [J]. Powder. Metall. Technol., 2013, 31: 89
|
|
方 彬, 纪 箴, 田高峰 等. FGH96高温合金中γ′相完全溶解温度的研究 [J]. 粉末冶金技术, 2013, 31: 89
|
| 21 |
Cui Z Q, Qin Y C. Metallography and Heat Treatment [M]. 2nd Ed., Beijing: China Machine Press, 2007: 202
|
|
崔忠圻, 覃耀春. 金属学与热处理 [M]. 第 2版, 北京: 机械工业出版社, 2007: 202
|
| 22 |
Kamaya M. Assessment of local deformation using EBSD: Quantification of accuracy of measurement and definition of local gradient [J]. Ultramicroscopy, 2011, 111: 1189
doi: 10.1016/j.ultramic.2011.02.004
pmid: 21763236
|
| 23 |
Hu J, Lin D L, Wang Y. EBSD analyses of the microstructural evolution and CSL characteristic grain boundary of coarse-grained NiAl alloy during plastic deformation [J]. Acta Metall. Sin., 2009, 45: 652
|
|
胡 静, 林栋樑, 王 燕. EBSD技术分析大晶粒NiAl合金高温塑性变形组织演变与CSL特征晶界分布 [J]. 金属学报, 2009, 45: 652
|
| 24 |
Wu J Q, Chen K, Chen X F, et al. Application of EBSD in the study of dynamic recrystallization mechanisms in Nimonic 80A [J]. J. Chin. Electron Microsc. Soc., 2011, 30: 356
|
|
吴洁琼, 陈 科, 陈杏芳 等. EBSD在Nimonic 80A动态再结晶机制研究中的应用 [J]. 电子显微学报, 2011, 30: 356
|
| 25 |
Mahajan S, Pande C S, Imam M A, et al. Formation of annealing twins in f.c.c. crystals [J]. Acta Mater., 1997, 45: 2633
|
| 26 |
Gleiter H. The mechanism of grain boundary migration [J]. Acta Metall., 1969, 17: 565
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|